IROGRAN® A 60 E 4902

About
IROGRAN A 60 E 4902 is a soft, high performance polyester based thermoplastic polyurethane intended for extrusion and moulding applications. IROGRANA 60 E 4902 is part of the HUNTSMAN Film and Sheet and Injection-Moulding product ranges. It is processable at low temperatures and offers a specially designed, flexible material suitable for elastic films & mouldings. PERFORMANCE FEATURES Excellent elasticity Excellent wear performance Good low temperature flexibility Enhanced Hydrolytic Stability Enhanced UV stability Low temperature processability&&

Product Description
SupplierHuntsman
GenericTPU-酯
Material StatusCommercial: Active
FeaturesWeather resistance is good,Excellent Processability,Good flexibility,High elastic,Hydrolysis stability,Low temperature toughness,Good wear resistance,Soft
AvailabilitysNorth America,Europe
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.14g/cm³ASTM D792
Density1.14g/cm³DIN 53478
Melt Volume Rate
160℃,8.7 kg35.0cm³/10min

MECHANICALNominal valueUnitTest method
Shore hardness DIN 53505
Shaw A, injection molding55 DIN 53505
Shaw’s D, injection molding15 DIN 53505
Shore hardness ASTM D2240
Shaw A, injection molding56 ASTM D2240
Shaw’s D, injection molding15 ASTM D2240
Wear amount 
43mm³DIN 53516
43mm³ASTM D395

elastic bodyNominal valueUnitTest method
Tensile Set(200% Strain)8%ASTM D412
Tensile Set(200% Strain)8%DIN 53504
tensile strength
Fracture, 0.635 mm7.52MPaASTM D412
Fracture, 0.635 mm10.0MPaDIN 53504
300% strain, 0.635 mm2.40MPaDIN 53504
300% strain, 0.635 mm4.07MPaASTM D412
100% strain, 0.635 mm1.40MPaDIN 53504
100% strain, 0.635 mm2.34MPaASTM D412
Tensile strain
Fracture, 0.635 mm900%DIN 53504
Fracture, 0.635 mm720%ASTM D412
tear strength
0.635 mm25kN/mDIN 53515
0.635 mm35.9kN/mASTM D624
Compression deformation ASTM D395
23℃,70 hr40%ASTM D395
70℃,24 hr80%ASTM D395
Compression deformation DIN 53517
23℃,70 hr35%DIN 53517
70℃,24 hr60%DIN 53517
Basho’s elasticity60%ASTM D2632

THERMALNominal valueUnitTest method
Melting temperature98.9 to 130Internal Method
TMA Internal Method
High:635.0 µm145Internal Method
Low:635.0 µm110Internal Method

Process Conditions
injectionNominal valueUnitTest method
ExtrusionNominal valueUnitTest method
Drying temperature – vacuum dryer40°C
Drying time – vacuum dryer4.0hr
Dew Point-30°C
Barrel rear temperature160 to 171°C
Barrel middle temperature160 to 171°C
Barrel front temperature160 to 171°C
Nozzle temperature160 to 171°C
Drying temperature40°C
Drying time4.0hr
Barrel 1 zone temperature160 to 171°C
Barrel 2 zone temperature160 to 171°C
Barrel 3 zone temperature160 to 171°C
Barrel 4 zone temperature160 to 171°C
Barrel 5 zone temperature160 to 171°C
Connector temperature160 to 171°C
Nozzle temperature160 to 171°C

Notes
1. Typical properties: these are not to be construed as specifications.
2. Injection Molded
3. Extruded Film, 0.025 in
4. Extruded Film
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.