TAROLOX 111 G6 DX0

About
PET glass fiber reinforced 30%, self extinguishing V0 without PBDE/PBDF, good flame proofing also at low thickness, high temperature resistance, good flow, very good mechanical, thermal and electrical properties, low moisture absorption, good dimensional stability. Product must be dryed before moulding. Available: different colors, release agent (W).&&

Product Description
GenericPET
Material StatusCommercial: Active
FeaturesGood Dimensional Stability,Good Electrical Properties,Good liquidity,Good stripping performance,Flame Characteristics,High Heat Resistance,Self-extinguishing,Low moisture absorption,V-0
AvailabilitysEurope
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.66 to 1.68g/cm³ASTM D792 , ISO 1183
Shrinkage rate ASTM D955
MD0.20 to 0.30%ASTM D955
TD0.50 to 0.70%ASTM D955
Water absorption rate
23℃,24hr0.050%ASTM D570,ISO 62
Granule Humidity< 0.030%Internal Method

IMPACTNominal valueUnitTest method
Charpy Notched Impact Strength
23℃9.0kJ/m²ASTM D256,ISO 179
Charpy Unnotch Impact strength
23℃46kJ/m²ASTM D256,ISO 179
Impact strength of cantilever beam notch ASTM D256 , ISO 180
-20℃,3.2mm70J/mASTM D256,ISO 180
23℃,3.2mm85J/mASTM D256,ISO 180

THERMALNominal valueUnitTest method
Hot deformation temperature 
0.45 MPa, unannealed246ASTM D648,ISO 75-2/B
1.8 MPa, unannealed225ASTM D648,ISO 75-2/A
Continuous use temperature 
150UL 746B
150IEC 60216
Vicat Softening Temp
B50240ISO 306/B50 , ASTM D1525 4
Ball pressure test
245℃通过 VDE 0470
Melting temperature256ASTM D211,ISO 121
Linear coefficient of thermal expansion
MD:-30~30℃2.0E-51/℃ASTM D696

Electrical performanceNominal valueUnitTest method
Volume resistivity1.0E+15ohms·cmASTM D257
Dielectric strength
1 mm32kV/mmASTM D149
Compared to the leakage tracing index
Solution A250VIEC 60112

FLAME CHARACTERISTICSNominal valueUnitTest method
Flame retardant level UL 94
1.00 mmV-0 UL 94
1.60 mmV-0 UL 94
3.20 mmV-0 UL 94
Igniting temperature of the hot wire
2 mm960IEC 60695-2-13
Extreme oxygen index32%ASTM D2863

MECHANICALNominal valueUnitTest method
Rockwell hardness
R-level120 ASTM D785
Tensile modulus11000MPaASTM D638 , ISO 527-2
tensile strength
fracture135MPaASTM D638 , ISO 527-2
Tensile strain
fracture2.0%ASTM D638 , ISO 527-2
Bending modulus10000MPaASTM D790 , ISO 178
bending strength 
220MPaISO 178
fracture220MPaASTM D790

Process Conditions
injectionNominal valueUnitTest method
Drying temperature  
110 to 130°C
Pre-drying equipment130 to 150°C
Processing (melt) temperature260 to 290°C
Mold temperature90 to 130°C
Injection speed中等偏快 

Notes
1. Typical properties: these are not to be construed as specifications.
2. 6x4x50 mm
3. 20000 hrs
4. Rate A (50°C/h), Loading 2 (50 N)
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.