SABIC® PPcompound 8650U

About
SABIC® PPcompound 8650U a development grade, elastomer-modified mineral filled Polypropylene for automotive exterior applications. This material combines excellent stiffness and high impact with low density. The combination makes the material very suitable for thin wall bumper applications. This grade is UV stabilized and can be used for unpainted applications. This grade will also be available in an open concept (8650 MB1 & 8650 MB2) and for painted applications (8650). SABIC® PPcompound 8650U is a designated automotive grade.&&

Product Description
SupplierSABIC
GenericPP not specified
Material StatusCommercial: Active
FeaturesGood Rigidity,Weather resistance is good,High impact resistance,Low density
AvailabilitysEurope
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density0.970g/cm³ISO 1183
Melt Flow Rate
230℃,2.16kg25g/10minISO 1133
Shrinkage rate
3.2 mm,24 hrs0.70 to 0.80%Internal Method

MECHANICALNominal valueUnitTest method
Tensile modulus
injection molding1500MPaISO 527-2/1B
tensile strength ISO 527-2/1A
Yield, injection molding18.0MPaISO 527-2/1A
Fracture, injection molding15.0MPaISO 527-2/1A
Tensile strain
Fracture, injection molding60%ISO 527-2/1A
Bending modulus
injection molding1550MPaASTM D790

IMPACTNominal valueUnitTest method
Impact strength of cantilever beam notch ISO 180/4A
-20 ℃, injection molding8.0kJ/m²ISO 180-4A
0 ℃, injection molding15kJ/m²ISO 180-4A
23 ℃, injection molding无断裂 ISO 180/4A

THERMALNominal valueUnitTest method
Linear coefficient of thermal expansion
MD:-30~100℃7.0E-51/℃ASTM D696

Notes
1. Typical properties: these are not to be construed as specifications.
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.