Egyeuroptene PP 9003 Improved Polypropylene, Homopolymer. Is a medium flow homopolymer with a conventional molecular weight distribution and is formulated with a general-purpose additive package. PP 9003 is designed for the production of films that can be converted into stretched tapes for weaving applications. Additional properties: suitable for the production of articles for food contact use. all other components used in the formulation meet the relevant fda requirements should not be assumed for other variants and should be investigated with the appropriate supply source.&& |
Product Description | |
---|---|
Generic | PP homopolymerization |
Material Status | Commercial: Active |
Features | Food contact compliance,Moderate liquidity,Homopolymer |
Availabilitys | Africa & Middle East ,Europe |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.900 | g/cm³ | ISO 1183/D |
Melt Flow Rate | |||
230℃,2.16kg | 3.0 | g/10min | ISO 1133 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Impact strength of cantilever beam notch | |||
23℃ | 4.0 | kJ/m² | ISO 180-1A |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
0.45 MPa, unannealed | 82.0 | ℃ | ISO 75-2/B |
1.8 MPa, unannealed | 51.0 | ℃ | ISO 75-2/A |
Vicat Softening Temp | |||
A50 | 155 | ℃ | ISO 306/A50 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Shore hardness | |||
Shaw’s D | 73 | ISO 868 | |
tensile strength | |||
yield | 33.0 | MPa | ISO 527-1-2 |
Bending modulus | 1400 | MPa | ISO 178 |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |