About |
---|
BC8360 is a two-part polyurethane molding system. BC8360 is mixed one-to-one by volume (or 100A-to-95B by weight) and cures at room temperature. BC8360 contains no fillers and cures to a firm (Shore A60 ± 4), medium amber rubber. Applications BC8360 is used to make molds of detailed masters that contain shallow undercuts. Some of the most common uses are concrete formliners and to make molds for point-of-purchase displays, rapid prototypes, special effects, taxidermy, and sculpture reproductions.&& |
Product Description | |
---|---|
Generic | PUR |
Material Status | Commercial: Active |
Features | Room Temperature Cure |
Availabilitys | North America |
Technical Data | |||
---|---|---|---|
THERMAL | Nominal value | Unit | Test method |
stripping time | |||
24℃ | 960 | min |
Uncured Properties | Nominal value | Unit | Test method |
---|---|---|---|
colour | |||
— | Amber | ||
— | Clear/Transparent | ||
Weight Mix Ratio (PBW) | |||
Part A | 100 | ||
Part B | 95 | ||
Volume Mixing Ratio (PBV) | |||
Part A | 1.0 | ||
Part B | 1.0 | ||
Density | |||
24℃ | 1.02 | g/cm³ | |
24℃ | 1.07 | g/cm³ | |
viscosity | |||
24℃ | 0.60 | Pa·s | |
24℃ | 2.3 | Pa·s | |
Curing time | |||
24℃ | 24 | hr | |
Gelation time | |||
24℃ | 20 to 30 | min | |
storage stability | |||
24 ℃ | 20 | min |
Cured Properties | Nominal value | Unit | Test method |
---|---|---|---|
Shore hardness | |||
Shaw’s A | 56 to 64 | ||
Tensile fracture strength | 5.17 | MPa | |
Tensile strain | |||
fracture | 500 | % | |
tear strength | |||
— | 5.25 | kN/m | |
Die C | 26.3 | kN/m | |
Resilience | 60 | % |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. Part B |
3. Part A |
4. Split |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |