About |
---|
M3804RW/RWP is a linear-low density polyethylene with a balance of impact properties, stiffness, and processability. M3804RW/RWP is suitable for rotational molding of storage tanks and general applications. It contains high level of UV stabilizer to give protection for outdoor use.&& |
Product Description | |
---|---|
Supplier | SCG |
Generic | Linear low density polyethylene |
Material Status | Commercial: Active |
Features | Good Rigidity,Weather resistance is good,Excellent Processability,High impact resistance,Food contact compliance |
Availabilitys | North America,Asia Pacific |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.938 | g/cm³ | ASTM D1505 |
Melt Flow Rate | |||
190℃,2.16kg | 4.0 | g/10min | ASTM D1238 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
ARM impact (-40 ℃) | 94.9 | J | ARM |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
1.8 MPa, unannealed | 70.0 | ℃ | ASTM D648 |
Embrittlement temperature | < -60.0 | ℃ | ASTM D746 |
Vicat Softening Temp | 120 | ℃ | ASTM D1525 |
Melting temperature | 125 | ℃ | ASTM D2117 |
Crystallization point | 113 | ℃ | ASTM D2117 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Shore hardness | |||
Shaw’s D | 60 | ASTM D2240 | |
tensile strength | ASTM D638 | ||
yield | 20.0 | MPa | ASTM D638 |
fracture | 18.0 | MPa | ASTM D638 |
Tensile strain | |||
fracture | 800 | % | ASTM D638 |
Bending modulus | |||
TD | 700 | MPa | ASTM D790 |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. 2.0 in/min |
3. 0.079 in/min |
4. 5 mm rotomolded sample |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |