IROGRAN A 85 P 4350 is a flame-retardant, halogen-free, thermoplastic polyether-polyurethane intended for extrusion and injection moulding applications. Additional characteristics of the product are excellent microbial resistance, high low-temperature flexibility, especially suitable for cable jackets. PERFORMANCE FEATURES Excellent hydrolysis resistance High microbial resistance High elasticity Flame retardant Halogen-free Good melt flow UL 94 classification V2 APPLICATIONS Cables Hoses Profiles Spiral Hoses&&

Product Description
SupplierHuntsman
GenericTPU-醚
Material StatusCommercial: Active
FeaturesHigh elastic,Hydrolysis stability,Good liquidity,Antimicrobial properties,Halogen free,Flame Characteristics,Low temperature toughness,V-2
AvailabilitysNorth America,Europe
Process MethodsExtrusion

Technical Data
PHYSICALNominal valueUnitTest method
Density1.15g/cm³
Density1.15g/cm³ISO 1183
Melt Volume Rate
190℃,21.6 kg50.0cm³/10min
Shrinkage rate
MD: Injection molding0.80%ASTM D955

MECHANICALNominal valueUnitTest method
Shore hardness ISO 868
Shaw A, injection molding87 ISO 868
Shaw’s D, injection molding36 ISO 868
Shore hardness ASTM D2240
Shaw A, injection molding87 ASTM D2240
Shaw’s D, injection molding36 ASTM D2240
Abrasion35mm³ISO 4649

elastic bodyNominal valueUnitTest method
tensile strength
fracture40.0MPaDIN 53504
fracture25.0MPaASTM D412
300% strain11.0MPaDIN 53504
300% strain10.0MPaASTM D412
100% strain7.00MPaASTM D412
100% strain6.50MPaDIN 53504
Tensile strain
fracture550%ASTM D412
fracture680%DIN 53504
tear strength80.6kN/mASTM D624
tear strength50kN/mISO 34-1
Compression deformation ASTM D395
23℃,24 hr25%ASTM D395
70℃,24 hr45%ASTM D395
Compression deformation ISO 815
23℃,24 hr25%ISO 815
70℃,24 hr45%ISO 815

THERMALNominal valueUnitTest method
TMA Internal Method
High:635.0 µm198Internal Method
Low:635.0 µm171Internal Method

FLAME CHARACTERISTICSNominal valueUnitTest method
Flame retardant levelV-2 UL 94

Process Conditions
injectionNominal valueUnitTest method
ExtrusionNominal valueUnitTest method
Drying temperature  
100 to 110°C
Hot Air Dryer80 to 90°C
Drying time  
3.0hr
Hot Air Dryer3.0hr
Dew Point-30°C
Barrel rear temperature175 to 195°C
Barrel middle temperature175 to 195°C
Barrel front temperature175 to 195°C
Nozzle temperature180 to 200°C
Processing (melt) temperature170 to 195°C
Mold temperature20 to 70°C
Drying temperature100 to 110°C
Drying time3.0hr
Hopper temperature25 to 40°C
Barrel 1 zone temperature165 to 190°C
Barrel 2 zone temperature165 to 190°C
Barrel 3 zone temperature165 to 190°C
Barrel 4 zone temperature165 to 190°C
Barrel 5 zone temperature165 to 190°C
Connector temperature175 to 195°C
Nozzle temperature175 to 200°C

Notes
1. Typical properties: these are not to be construed as specifications.
2. Injection Molded
3. Extruded Film
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.