About |
---|
Multi-Flex® TPE A7204 LC is a Thermoplastic Elastomer (TPE) product. It is available in Africa & Middle East, Asia Pacific, Europe, Latin America, or North America.&& |
Product Description | |
---|---|
Generic | TPE |
Material Status | Commercial: Active |
Features | Good Dimensional Stability |
Availabilitys | Africa & Middle East ,North America,Latin America,Asia Pacific,Europe |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.07 | g/cm³ | ASTM D792 |
Melt Flow Rate | |||
230℃,2.16kg | 0.70 | g/10min | ASTM D1238 |
elastic body | Nominal value | Unit | Test method |
---|---|---|---|
tensile strength | |||
fracture | 11.0 | MPa | ASTM D412 |
Tensile strain | |||
fracture | 600 | % | ASTM D412 |
tear strength | 35.0 | kN/m | ASTM D624 |
Compression deformation | ASTM D395 | ||
23℃,22 hr | 13 | % | ASTM D395 |
70℃,22 hr | 33 | % | ASTM D395 |
100℃,22 hr | 55 | % | ASTM D395 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Shore hardness | |||
Shore A, 10 seconds | 69 | ASTM D2240 |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Extrusion | Nominal value | Unit | Test method |
Drying temperature | 66 | °C | |
Drying time | 2.0 to 4.0 | hr | |
Barrel rear temperature | 191 | °C | |
Barrel middle temperature | 196 | °C | |
Barrel front temperature | 202 | °C | |
Nozzle temperature | 202 | °C | |
Processing (melt) temperature | 202 | °C | |
Mold temperature | 27 to 43 | °C | |
Injection speed | Moderate-Fast | ||
Barrel 1 zone temperature | 160 | °C | |
Barrel 3 zone temperature | 188 | °C | |
Barrel 5 zone temperature | 210 | °C | |
Melt temperature | 204 | °C | |
Nozzle temperature | 213 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |