LEXAN™ HF1110R resin

About
High flow grade. Easy mold release version of LEXAN HF1110. For thin wall lighting lenses, data storage components and safety eyewear lenses.&&

Product Description
SupplierSABIC
GenericPolycarbonate
Material StatusCommercial: Active
FeaturesExcellent Processability,High liquidity,Good stripping performance,V-2
AvailabilitysNorth America,Asia Pacific,Europe
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.20g/cm³ASTM D792
Melt Flow Rate
300℃,1.20kg25g/10minASTM D1238
Shrinkage rate
MD:3.2 mm0.50 to 0.70%Internal Method

MECHANICALNominal valueUnitTest method
tensile strength
fracture65.5MPaASTM D638
yield62.1MPaASTM D638
Tensile strain
fracture120%ASTM D638
Bending modulus
50 mm span2310MPaASTM D790
bending strength
Yield, 50 mm span93.1MPaASTM D790

IMPACTNominal valueUnitTest method
Impact strength of cantilever beam notch
23℃640J/mASTM D256
Dart impact equipped with measuring instruments
23℃,Energy at Peak Load54.2JASTM D3763
Tensile impact strength378kJ/m²ASTM D1822

THERMALNominal valueUnitTest method
Hot deformation temperature
1.8 MPa, unannealed, 3.2 mm127ASTM D648
Relative temperature index
Electrical performance130UL 746
Strength mechanical performance130UL 746
Impact mechanical performance130UL 746

Electrical performanceNominal valueUnitTest method
Compared to the leakage tracing indexPLC 2 UL 746
High Arc Burning Index (HAI)PLC 1 UL 746
High voltage arc marking rate
HVTRPLC 2 UL 746
Hot wire ignition
HWIPLC 2 UL 746

FLAME CHARACTERISTICSNominal valueUnitTest method
1.10 mmV-2 UL 94

optical performanceNominal valueUnitTest method
Transmittance
2540 µm88.0%ASTM D1003
Haze
2540 µm1.0%ASTM D1003

Process Conditions
InjectionNominal valueUnitTest method
drying temperature121°C
Drying time3.0 to 4.0hr
Drying time, maximum48hr
Recommended maximum moisture content0.020%
Suggested injection volume40 to 60%
Temperature at the rear of the barrel249 to 271°C
Temperature in the middle of the barrel260 to 282°C
Front temperature of material barrel271 to 293°C
Nozzle temperature266 to 288°C
Processing (melt) temperature271 to 293°C
Mold temperature71 to 93°C
Back pressure0.345 to 0.689MPa
Screw speed40 to 70rpm
Exhaust hole depth0.025 to 0.076mm

Notes
1. Typical properties: these are not to be construed as specifications.
2. Type I, 2.0 in/min
3. 0.051 in/min
4. Type S
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.