TAROMID A 280 H G6 X0

About
Polyamide 66 medium viscosity, 30% glass fiber reinforced, UL94 V0 self extinguishing, heat stabilized, very good flame proofing also at low thickness. High mechanical and thermal properties, low shrinkage and high dimensional stability, high tracking resistance. Material PBDE/PBDF free. UL94 V0 approved – All color at 0,88 mm – NC,BK, thickness 0,75 mm – UL 746B approved – CTI UL94 class 1. Available: different colors, release agent (W).&&

Product Description
GenericPA66
Material StatusCommercial: Active
FeaturesGood Dimensional Stability,Low contractility,Good stripping performance,Flame Characteristics,Self-extinguishing,Heat Stabilized,Electric mark,V-0
AvailabilitysEurope
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.56 to 1.58g/cm³ASTM D792 , ISO 1183
Shrinkage rate ASTM D955
MD:3.2 mm0.30 to 0.50%ASTM D955
TD:3.2 mm0.45 to 0.75%ASTM D955
Water absorption rate ASTM D570 , ISO 62
23℃,24hr0.50%ASTM D570,ISO 62
Saturation, 23 ℃4.5%ASTM D570,ISO 62
Granule Humidity< 0.15%Internal Method

IMPACTNominal valueUnitTest method
Charpy Notched Impact Strength
23℃7.2kJ/m²ASTM D256,ISO 179
Impact strength of cantilever beam notch
23℃,3.2mm75J/mASTM D256,ISO 180

THERMALNominal valueUnitTest method
Hot deformation temperature 
1.8 MPa, unannealed, 3.2 mm240ASTM D648
1.8 MPa, unannealed240ISO 75-2/A
Continuous use temperature 
100UL 746B
120UL 746B
140UL 746B
180IEC 60216
Vicat Softening Temp
B50242ISO 306/B50 , ASTM D1525 10
Ball pressure test
205℃通过 VDE 0470
Melting temperature250 to 256ASTM D211,ISO 121
Linear coefficient of thermal expansion
MD:-30~30℃2.8E-51/℃ASTM D696

Electrical performanceNominal valueUnitTest method
Volume resistivity1.0E+15ohms·cmASTM D257
Dielectric strength
2 mm26kV/mmASTM D149
Compared to the leakage tracing index
Solution A> 400VIEC 60112

FLAME CHARACTERISTICSNominal valueUnitTest method
Flame retardant level UL 94
0.75 mm, natural color, blackV-0 UL 94
0.90 mm, all colorsV-0 UL 94
Glowing wire flammability index
1.2 mm850IEC 60695-2-12
Igniting temperature of the hot wire
1.2 mm775IEC 60695-2-13
Extreme oxygen index30%ASTM D2863

MECHANICALNominal valueUnitTest method
Rockwell hardness
R-level122 ASTM D785
Tensile modulus9200MPaASTM D638 , ISO 527-2
tensile strength
fracture145MPaASTM D638 , ISO 527-2
Tensile strain
fracture2.2%ASTM D638 , ISO 527-2
Bending modulus9000MPaASTM D790 , ISO 178
bending strength 
200MPaISO 178
fracture200MPaASTM D790

Process Conditions
injectionNominal valueUnitTest method
Drying temperature  
80 to 90°C
Pre-drying equipment80 to 100°C
Drying time  
1.0hr
Pre-drying equipment3.0hr
Processing (melt) temperature260 to 270°C
Mold temperature80 to 110°C

Notes
1. Typical properties: these are not to be construed as specifications.
2. 6x4x50 mm
3. M. with imp.0,75 mm
4. M. with imp. 3 mm
5. E. 0,75 mm
6. M. w/o imp. 3 mm
7. M. w/o imp.0,75 mm
8. Short Term
9. Rate B (120°C/h), Loading 2 (50 N)
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.