About |
---|
TechnoFiber: Strong and light TechnoFiber products are long glass fiber remforced thermoplastics made by TechnoCompound GmbH. These raw materials are fashioned into so-called tailor-made compounds upon customer specifications. Nearly all semi-crystalline and amorphous thermoplastics can be used as thermoplastic matrlx. Our long glass flber products are predestmed for the manufacturing of components which are exposed to extreme mechanical stress – as well as to high temperatures. The long glass fiber reinforced pellets are available in lengths of 10 – 25 mm. Fiber and pellet are of the same length. The two-step pultrusion technology applied by TechnoCompound coats each glass flber fllament wlth a polymer matrrx and JOINS flber and matrrx. Typical Applications Automobil: Automotive industry: battery holders, wheel covers, ash trays, engine insulation, gear shift sticks, electronic accelerator pedals, exhaust trims, instrument panel… Electrical engineering: casings for power tools… Leisure industry: snowboard bindings… Construction industry: wear-resistant conveyor belts Furniture industry: fittings, chair frames, hinges…&& |
Product Description | |
---|---|
Generic | PP not specified |
Material Status | Commercial: Active |
Features | Good Rigidity,Weather resistance is good,High impact resistance,High Heat Resistance,Low odor,Hypocrystalline,Amorphous |
Availabilitys | North America,Asia Pacific,Europe |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.20 | g/cm³ | ISO 1183 |
Shrinkage rate | |||
MD | 0.20 | % | ISO 294-4 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Tensile modulus | 8700 | MPa | ISO 527-1-2 |
tensile strength | |||
yield | 115 | MPa | ISO 527-2/50 |
Tensile strain | |||
yield | 2.5 | % | ISO 527-2/50 |
Bending modulus | 8900 | MPa | ISO 178 |
bending strength | 130 | MPa | ISO 178 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | ||
-30℃ | 21 | kJ/m² | ISO 179/1eA |
23℃ | 20 | kJ/m² | ISO 179/1eA |
Charpy Unnotch Impact strength | ISO 179/1eU | ||
-30℃ | 58 | kJ/m² | ISO 179/1eU |
23℃ | 58 | kJ/m² | ISO 179/1eU |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
0.45 MPa, unannealed | 160 | ℃ | ISO 75-2/B |
1.8 MPa, unannealed | 150 | ℃ | ISO 75-2/A |
8.0 MPa, unannealed | 124 | ℃ | ISO 75-2/C |
Melting temperature | 165 | ℃ | ISO 11357-3 |
Linear coefficient of thermal expansion | ISO 11359-2 | ||
MD:23~80℃ | 1.5E-5 | 1/℃ | ISO 11359-2 |
TD:23~80℃ | 3.4E-5 | 1/℃ | ISO 11359-2 |
Notes |
---|
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |