| About |
|---|
| Flame-retarded V0-rated PBT/ABS alloy&& |
| Product Description | |
|---|---|
| Supplier | LTL Color |
| Generic | ABS+PBT |
| Material Status | Commercial: Active |
| Features | Flame Characteristics,V-0 |
| Availabilitys | Africa & Middle East ,North America,Latin America,Asia Pacific,Europe |
| Process Methods | Injection Molding |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 1.30 | g/cm³ | ASTM D792 |
| MECHANICAL | Nominal value | Unit | Test method |
|---|---|---|---|
| tensile strength | |||
| fracture | 39.3 | MPa | ASTM D638 |
| yield | 42.1 | MPa | ASTM D638 |
| Tensile strain | |||
| fracture | 13 | % | ASTM D638 |
| Bending modulus | 2210 | MPa | ASTM D790 |
| bending strength | 68.9 | MPa | ASTM D790 |
| IMPACT | Nominal value | Unit | Test method |
|---|---|---|---|
| Impact strength of cantilever beam notch | |||
| 23℃ | 53 | J/m | ASTM D256 |
| FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
|---|---|---|---|
| 1.40 mm | V-0 | UL 94 |
| Process Conditions | |||
|---|---|---|---|
| injection | Nominal value | Unit | Test method |
| Drying temperature | 85 | °C | |
| Drying time | 3.0 to 4.0 | hr | |
| Drying time, maximum | 8.0 | hr | |
| Recommended injection volume | 40 to 60 | % | |
| Barrel rear temperature | 204 to 238 | °C | |
| Barrel middle temperature | 210 to 232 | °C | |
| Barrel front temperature | 221 to 254 | °C | |
| Nozzle temperature | 216 to 249 | °C | |
| Processing (melt) temperature | 221 to 254 | °C | |
| Mold temperature | 10 to 71 | °C | |
| Back pressure | 0.345 to 0.689 | MPa | |
| Screw speed | 40 to 70 | rpm | |
| Vent depth | 0.025 to 0.076 | mm | |
| Notes |
|---|
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |