About |
---|
Advanced Composites BJS-MNR2 is a Polypropylene product. It is available in North America. Characteristics include: Copolymer Impact Resistant&& |
Product Description | |
---|---|
Generic | PP not specified |
Material Status | Commercial: Active |
Features | High impact resistance,Impact copolymer |
Availabilitys | North America |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.900 | g/cm³ | ASTM D792 |
Melt Flow Rate | |||
230℃,2.16kg | 12 | g/10min | ASTM D1238 |
Shrinkage rate | |||
MD:3.0 mm | 1.4 to 1.7 | % | ASTM D955 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Impact strength of cantilever beam notch | |||
23℃ | 无断裂 | ASTM D256 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
0.45 MPa, unannealed | 88.0 | ℃ | ASTM D648 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Rockwell hardness | |||
R-level | 75 | ASTM D785 | |
tensile strength | |||
yield | 23.3 | MPa | ASTM D638 |
Tensile strain | |||
fracture | 300 | % | ASTM D638 |
Bending modulus | 950 | MPa | ASTM D790 |
bending strength | 23.3 | MPa | ASTM D790 |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Barrel rear temperature | 199 | °C | |
Barrel middle temperature | 210 to 221 | °C | |
Barrel front temperature | 221 | °C | |
Nozzle temperature | 216 | °C | |
Processing (melt) temperature | 185 to 227 | °C | |
Mold temperature | 27 to 43 | °C | |
Injection speed | 慢to中等 | ||
Cushion | 5.00 to 10.0 | mm |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. 0.39 in/min |
3. 0.079 in/min |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |