| About |
|---|
| POLYSTYRENE (PS) COMPOUNDS (CPDS) FT876 is a high impact, halogen free flame retardant polystyrene with good thermal stability and process ability Main Characteristics Bromine and Chlorine free UL94 V0 @ 2.5 mm. High heat and good thermal and UV stability Applications Television covers, decoders, Hi-Fi. Office automation.&& |
| Product Description | |
|---|---|
| Supplier | TOTAL |
| Generic | PS (IRPS) |
| Material Status | Commercial: Active |
| Features | Weather resistance is good,Excellent Processability,High impact resistance,Halogen free,Flame Characteristics,High Heat Resistance,Heat Stabilized,V-0 |
| Availabilitys | Europe |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 1.10 | g/cm³ | ISO 1183 |
| Apparent density | 0.60 | g/cm³ | |
| Melt Flow Rate | |||
| 200℃,5.0kg | 3.0 | g/10min | ISO 1133 |
| Shrinkage rate | 0.40 to 0.70 | % | |
| Water absorption rate | |||
| Equilibrium, 23 ℃, 50% RH | < 0.10 | % | ISO 62 |
| MECHANICAL | Nominal value | Unit | Test method |
|---|---|---|---|
| tensile strength | ISO 527-2 | ||
| yield | 30.0 | MPa | ISO 527-2 |
| fracture | 40.0 | MPa | ISO 527-2 |
| Tensile strain | |||
| fracture | 40 | % | ISO 527-2 |
| Bending modulus | 2300 | MPa | ISO 178 |
| IMPACT | Nominal value | Unit | Test method |
|---|---|---|---|
| Impact strength of cantilever beam notch | |||
| 23℃ | 6.0 | kJ/m² | ISO 180-1A |
| THERMAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Vicat Softening Temp | |||
| B50 | 85.0 | ℃ | ISO 306 |
| FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
|---|---|---|---|
| 2.5 mm,Black & Gray | V-0 | UL 94 |
| Notes |
|---|
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |