Quadraflex™ ARE-93A is high performance aromatic polyether thermoplastic polyurethane. The polymer is naturally clear and supplied in small pellets for ease of processing. The material exhibits excellent mechanical properties, oxidative stability, biocompatibility, elasticity, chemical resistance, high resliency and softening at body temperature. The resin has consistent melt flow properties making it ideal for extrusion. Quadrathane™, Quadraflex™, Quadraban™ and Quadraplast™ performance polymers are primarily used in life science and medical applications including vascular access devices, surgical supplies, respiratory devices, tracheotomy devices, and other medical applications. Typical end products include tubing, catheter parts, balloons, and various medical device components. These performance polymers are available in a variety of durometers, radiopacifiers, colors, and custom formulations.&& |
Product Description | |
---|---|
Generic | TPU-醚 |
Material Status | Commercial: Active |
Features | Excellent Processability,High elastic,Good liquidity,Aromatic,Biocompatible,Inoxidizability,Elastic,Solvent resistance |
Availabilitys | North America |
Process Methods | Extrusion |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.15 | g/cm³ | ASTM D792 |
Melt Flow Rate | |||
190℃,2.16kg | 7.5 | g/10min | ASTM D1238 |
Shrinkage rate | |||
MD | 0.50 to 0.80 | % | ASTM D955 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Shore hardness | |||
Shaw’s A | 93 | ASTM D2240 |
elastic body | Nominal value | Unit | Test method |
---|---|---|---|
tensile strength | ASTM D412 | ||
fracture | 41.4 | MPa | ASTM D412 |
100% strain | 8.27 | MPa | ASTM D412 |
300% strain | 13.8 | MPa | ASTM D412 |
Tensile strain | |||
fracture | 500 | % | ASTM D412 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Post curing time | |||
38℃ | 6.0 to 10 | hr |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Extrusion | Nominal value | Unit | Test method |
Drying temperature | 54 | °C | |
Drying time | 4.0 | hr | |
Recommended maximum moisture content | < 3.0E-3 | % | |
Barrel rear temperature | 177 | °C | |
Barrel front temperature | 191 | °C | |
Nozzle temperature | 196 | °C | |
Processing (melt) temperature | 204 | °C | |
Mold temperature | 4 to 32 | °C | |
Drying temperature | 54 | °C | |
Drying time | 4.0 | hr | |
Recommended maximum moisture content | < 0.030 | % | |
Barrel 1 zone temperature | 171 | °C | |
Barrel 2 zone temperature | 182 | °C | |
Barrel 3 zone temperature | 188 | °C | |
Barrel 4 zone temperature | 193 | °C | |
Melt temperature | 193 | °C | |
Nozzle temperature | 193 to 216 | °C | |
Back pressure | 6.89 to 12.4 | MPa |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |