Baydur STR 822 is a polyurethane medium to high density structural RIM system used in the Long Fiber Injection (LFI) technology. The Baydur STR 822 system is used in an open mold process with varying levels of fiberglass reinforcement depending on the property requirements needed. The system has a long gel time, yet fast cure time, which makes it well suited for large part applications. The Baydur STR 822 system is supplied as two reactive liquid components. Component A is a polymeric diphenlymethane diisocyanate (PMDI), and Component B is a formulated polyether polyol system. As with any product, use of the Baydur STR 822 system in a given application must be tested (including field-testing, etc.) in advance by the user to determine suitability.&& |
Product Description | |
---|---|
Supplier | Covestro |
Generic | PUR+MDI |
Material Status | Commercial: Active |
Availabilitys | Africa & Middle East ,North America,Latin America,Asia Pacific,Europe |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.12 | g/cm³ |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
tensile strength | |||
5.05 mm | 58.2 | MPa | |
Tensile strain | |||
Fracture, 5.05 mm | 2.1 | % | |
Bending modulus | |||
5.05 mm | 5740 | MPa |
Supplementary information | Nominal value | Unit | Test method |
---|---|---|---|
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Linear coefficient of thermal expansion | |||
MD | 4.3E-5 | 1/℃ | ASTM D696 |
Thermosetting components | |||
Component A | 按重量计算的混合比: 230 | ||
Component B | 按重量计算的混合比: 100 |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |