Medalist™ MD-12140 (PRELIMINARY DATA)

About
The Medalist MD-12100 Series are high performance thermoplastic elastomers designed for medical and healthcare applications requiring high elasticity and excellent moldability. Medalist MD-12140 is a low hardness, low density grade, available in NAT and colors, which can be sterilized and exhibits excellent adhesion to polypropylene.&&

Product Description
SupplierTeknor Apex
GenericTPE
Material StatusCommercial: Active
FeaturesExcellent Processability,Good flexibility,Low liquidity,Smoothness,Good disinfection,Halogen free,High pressure disinfection,Good bond,Lubricating,Elastic,Low density,Radiation disinfection,Low Hardness,Solvent resistance,Ethylene oxide disinfection
AvailabilitysAfrica & Middle East ,North America,Latin America,Asia Pacific,Europe
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density0.883g/cm³ASTM D792
Melt Flow Rate
200℃,5.0kg7.0g/10minASTM D1238

MECHANICALNominal valueUnitTest method
Shore hardness ASTM D2240
Shore A, 1 second42 ASTM D2240
Shore A, 5 seconds40 ASTM D2240

elastic bodyNominal valueUnitTest method
tensile strength ASTM D412
fracture4.07MPaASTM D412
50% strain1.14MPaASTM D412
100% strain1.38MPaASTM D412
300% strain2.14MPaASTM D412
Tensile strain
fracture600%ASTM D412
tear strength21.7kN/mASTM D624
Compression deformation ASTM D395
23℃,22 hr16%ASTM D395
70℃,22 hr28%ASTM D395

Process Conditions
injectionNominal valueUnitTest method
Barrel rear temperature160 to 177°C
Barrel middle temperature182 to 204°C
Barrel front temperature193 to 216°C
Nozzle temperature182 to 227°C
Processing (melt) temperature182 to 227°C
Mold temperature27 to 49°C

Notes
1. Typical properties: these are not to be construed as specifications.
2. Die C, 20 in/min
3. Type 1
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.