Evoprene™ GC 082

About
Static Internal white. Window gasket.&&

Product Description
GenericTPE
Material StatusCommercial: Active
AvailabilitysNorth America,Europe

Technical Data
PHYSICALNominal valueUnitTest method
Density1.10g/cm³ISO 1183

MECHANICALNominal valueUnitTest method
Shore hardness
Shore A, 10 seconds, 6.50 mm56 ISO 868

elastic bodyNominal valueUnitTest method
tensile strength
Yield, 2 mm3.80MPaISO 37
100% strain, 2 mm2.30MPaISO 37
Tensile strain
Fracture, 2 mm490%ISO 37
tear strength
2.00 mm22kN/mISO 34-1
Compression deformation ISO 815
22℃,72 hr23%ISO 815
70℃,22 hr76%ISO 815
100℃,22 hr99%ISO 815

Aging performanceNominal valueUnitTest method
The rate of change in tensile strength in air
70℃,336 hr8.0%ISO 188
Changes in tensile stress during fracture in air
70℃,336 hr3.0%ISO 188
The rate of change of Shore hardness in air
Shore A, 70 ℃, 336 hr-1.0 ISO 188

Notes
1. Typical properties: these are not to be construed as specifications.
2. Method Ba, Angle (Unnicked)
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.