About |
---|
DISTRUMID 6 GF50是一种聚酰胺6(尼龙6)材料,。 该产品在欧洲有供货,。 DISTRUMID 6 GF50的主要特性为:阻燃/额定火焰。&& |
Product Description | |
---|---|
Generic | PA6 |
Material Status | Commercial: Active |
Features | HB |
Availabilitys | Europe |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.55 | g/cm³ | ASTM D792 |
Shrinkage rate | |||
MD | 0.20 | % | ASTM D955 |
Water absorption rate | |||
24hr | 0.70 | % | ASTM D570 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
1.8 MPa, unannealed | 215 | ℃ | ASTM D648 |
0.45 MPa, unannealed | 220 | ℃ | ASTM D648 |
Vicat Softening Temp | 210 | ℃ | ASTM D1525 |
Melting temperature | 222 | ℃ |
Electrical performance | Nominal value | Unit | Test method |
---|---|---|---|
Surface resistivity | 1.0E+13 | ohms | ASTM D257 |
Volume resistivity | 1.0E+15 | ohms·cm | ASTM D257 |
FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
---|---|---|---|
Flame retardant level | HB | UL 94 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
tensile strength | |||
limit | 190 | MPa | ASTM D638 |
Tensile strain | |||
fracture | 2.0 | % | ASTM D638 |
Bending modulus | 13000 | MPa | ASTM D790 |
Rockwell hardness | |||
R-level | 123 | ASTM D785 |
Notes |
---|
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |