Alcryn® ALR 7225

About
Alcryn® ALR 7225 MPR has improved heat resistance over standard Alcryn grades and has an upper temperature limit of 136°C, while retaining at least 85% of original tensile properties. ALR 7225 is designed for the extrusion process, specifically Wire & Cable applications and should be considered where increased temperature resistance is required.&&

Product Description
SupplierA. Schulman
GenericMPR
Material StatusCommercial: Active
FeaturesHigh Heat Resistance
AvailabilitysNorth America,Asia Pacific,Europe
Process MethodsExtrusion

Technical Data
PHYSICALNominal valueUnitTest method
Density1.30g/cm³ASTM D792
Density1.30g/cm³ISO 1183

elastic bodyNominal valueUnitTest method
tensile strength
yield9.64MPaISO 37
100% strain4.85MPaASTM D412
100% strain4.85MPaISO 37
Tensile strain
fracture370%ISO 37
fracture370%ASTM D412
tear strength
24℃39.8kN/mASTM D624
Compression deformation ASTM D395B
24℃,22 hr32%ASTM D395B
70℃,22 hr73%ASTM D395B
Compression deformation ISO 815
24℃,22 hr32%ISO 815
70℃,22 hr73%ISO 815

MECHANICALNominal valueUnitTest method
Shore hardness
Shaw’s A82 ISO 868
Shaw’s A82 ASTM D2240

Electrical performanceNominal valueUnitTest method
Surface resistivity7.3E+11ohmsASTM D257
Volume resistivity4.4E+11ohms·cmASTM D257
Dielectric strength
0.00191 mm0.45kV/mmASTM D149

Notes
1. Typical properties: these are not to be construed as specifications.
2. Die C
3. Type B
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.