About |
---|
RC Plastics RCPCA10 is a Polycarbonate + ABS (PC+ABS) product. It can be processed by injection molding and is available in North America. Characteristics include: Flame Rated Eco-Friendly/Green&& |
Product Description | |
---|---|
Generic | PC+ABS |
Material Status | Commercial: Active |
Features | V-0 |
Availabilitys | North America |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.19 | g/cm³ | ASTM D792 |
Melt Flow Rate | |||
260℃,2.16kg | 10 | g/10min | ASTM D1238 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
tensile strength | 59.3 | MPa | ASTM D638 |
Tensile strain | |||
fracture | 20 | % | ASTM D638 |
Bending modulus | 2620 | MPa | ASTM D790 |
bending strength | 92.4 | MPa | ASTM D790 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Notched impact strength of cantilever beam | 530 | J/m | ASTM D256 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
1.8 MPa, unannealed | 90.6 | ℃ | ASTM D648 |
FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
---|---|---|---|
Flame retardant level | UL 94 | ||
1.60 mm | V-0 | UL 94 | |
3.20 mm | V-0 | UL 94 |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Drying temperature | 82 | °C | |
Drying time | 3.0 to 4.0 | hr | |
Barrel rear temperature | 232 to 282 | °C | |
Barrel middle temperature | 232 to 282 | °C | |
Barrel front temperature | 232 to 282 | °C | |
Processing (melt) temperature | 221 to 288 | °C | |
Mold temperature | 49 to 79 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |