| About |
|---|
| ACRYMID 813 compound is an amorphous and heat-resistant thermoplastic molding compound based on polymethyl methacrylimide (PMMI). Typical properties of ACRYMID® heat-resistant molding compounds are: high light transmission high heat resistance very high strength and rigidity good weather resistance The special properties of ACRYMID 813 compound are: high melt flow rate AMECA listed Application: Used for injection molding parts that involve a high degree of thermal stress.&& |
| Product Description | |
|---|---|
| Supplier | Evonik |
| Generic | PMMI |
| Material Status | Commercial: Active |
| Features | Good Rigidity,Weather resistance is good,Good Clarity,High liquidity,High Heat Resistance,Amorphous |
| Availabilitys | North America,Europe |
| Process Methods | Injection Molding |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 1.21 | g/cm³ | ASTM D792 |
| Melt Flow Rate | |||
| 260℃,3.80kg | 16 | g/10min | ASTM D1238 |
| Shrinkage rate | |||
| MD | 0.80 to 0.90 | % | ASTM D955 |
| Water absorption rate | |||
| balance | < 0.30 | % | ASTM D570 |
| IMPACT | Nominal value | Unit | Test method |
|---|---|---|---|
| Impact strength of cantilever beam notch | |||
| 23℃,6.4mm | 13 | J/m | ASTM D256 |
| THERMAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Hot deformation temperature | |||
| 1.8 MPa, annealed, 6.35 mm | 122 | ℃ | ASTM D648 |
| Vicat Softening Temp | 126 | ℃ | ASTM D1525 |
| Linear coefficient of thermal expansion | |||
| MD:0~100℃ | 7.7E-5 | 1/℃ | ASTM D696 |
| optical performance | Nominal value | Unit | Test method |
|---|---|---|---|
| Transmittance | |||
| 3200 µm | 91.0 | % | ASTM D1003 |
| Haze | |||
| 3200 µm | < 1.0 | % | ASTM D1003 |
| Yellowness index | |||
| 3.20 mm | < 1.0 | YI | ASTM D1925 |
| MECHANICAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Rockwell hardness | |||
| M-level | 97 | ASTM D785 | |
| Tensile modulus | 4100 | MPa | ASTM D638 |
| tensile strength | 90.0 | MPa | ASTM D638 |
| Tensile strain | |||
| yield | 2.0 to 4.0 | % | |
| fracture | 2.0 to 4.0 | % | |
| Bending modulus | 3800 | MPa | ASTM D790 |
| bending strength | 137 | MPa | ASTM D790 |
| Process Conditions | |||
|---|---|---|---|
| injection | Nominal value | Unit | Test method |
| Drying temperature | 115 | °C | |
| Drying time | 2.0 to 3.0 | hr | |
| Barrel rear temperature | 250 to 280 | °C | |
| Barrel middle temperature | 250 to 280 | °C | |
| Barrel front temperature | 250 to 280 | °C | |
| Processing (melt) temperature | 250 to 280 | °C | |
| Mold temperature | 80 to 100 | °C | |
| Notes |
|---|
| 1. Typical properties: these are not to be construed as specifications. |
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |