| About |
|---|
| HIPTEN® 22020 is low density polyethylene resin developed for film extrusion. This grade has good mechanical and optical properties and good draw down characteristics. Film produced from this grade has good appearance and heat sealability, good moisture barrier and adhesion properties. Applications: Production of laminated food-packaging materials. HIPTEN® 22020 has Health Certificate issued by Institute for Health Protection of Serbia.&& |
| Product Description | |
|---|---|
| Generic | LDPE |
| Material Status | Commercial: Active |
| Features | Good surface appearance,Good heat sealing,Good dissection,Renewable resources,Optical performance,Food contact compliance,Good bond,Moisture resistance |
| Availabilitys | Asia Pacific,Europe |
| Process Methods | Film extrusion |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 0.921 | g/cm³ | ISO 1183 |
| Melt Flow Rate | |||
| 190℃,2.16kg | 2.0 | g/10min | ISO 1133 |
| film | Nominal value | Unit | Test method |
|---|---|---|---|
| film thickness | |||
| test | 40 | µm | |
| tensile strength | ISO 527-3 | ||
| TD, yield, 40 µ m, blow molded film | 12.0 | MPa | ISO 527-3 |
| MD, fracture, 40 µ m, blow molded film | 20.0 | MPa | ISO 527-3 |
| TD, fracture, 40 µ m, blow molded film | 19.0 | MPa | ISO 527-3 |
| Tensile strain | ISO 527-3 | ||
| fracture | 600 | % | ISO 527-2 |
| MD, fracture, 40 µ m, blow molded film | 650 | % | ISO 527-3 |
| TD, fracture, 40 µ m, blow molded film | 750 | % | ISO 527-3 |
| Drop hammer impact | |||
| 40 µm | 120 | g | ASTM D1709-A |
| tear strength | ASTM D1922 | ||
| MD,40 µm | 135.1 | kN/m | ASTM D1922 |
| TD,40 µm | 173.7 | kN/m | ASTM D1922 |
| THERMAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Vicat Softening Temp | 96.0 | ℃ | ISO 306 |
| MECHANICAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Shore hardness | |||
| Shaw’s D | 46 | ISO 868 | |
| tensile strength | ISO 527-2 | ||
| yield | 9.00 | MPa | ISO 527-2 |
| fracture | 12.0 | MPa | ISO 527-2 |
| Process Conditions | |||
|---|---|---|---|
| Extrusion | Nominal value | Unit | Test method |
| Melt temperature | 180 to 200 | °C | |
| Notes |
|---|
| 1. Typical properties: these are not to be construed as specifications. |
| 2. Blown Film |
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |