| About |
|---|
| Medalist MD-10308 is a high performance thermoplastic elastomer specifically designed for healthcare and medical applications. Medalist MD-10308 is a low hardness, low density, halogen-free grade that can be sterilized and is suitable for injection molding, extrusion, and cast film.&& |
| Product Description | |
|---|---|
| Supplier | Teknor Apex |
| Generic | TPE |
| Material Status | Commercial: Active |
| Features | Excellent Processability,Good Clarity,Good flexibility,High elastic,Halogen free,Low Hardness,Low odor,Good bond,Good melt strength,Elastic,Good Tensile Strength,Low density,Good tear strength,Solvent resistance,Soft,Puncture Resistant,Ethylene oxide disinfection,Good coloring |
| Availabilitys | Africa & Middle East ,North America,Latin America,Asia Pacific,Europe |
| Process Methods | Film extrusion |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 0.868 | g/cm³ | ASTM D792 |
| Melt Flow Rate | |||
| 190℃,2.16kg | 15 | g/10min | ASTM D1238 |
| MECHANICAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Shore hardness | |||
| Shore A, 1 second, injection molding | 10 | ||
| Shore A, 5 seconds, injection molding | 8 |
| elastic body | Nominal value | Unit | Test method |
|---|---|---|---|
| tensile strength | |||
| fracture | 4.24 | MPa | ASTM D412 |
| 100% strain | 0.207 | MPa | |
| 300% strain | 0.414 | MPa | |
| Tensile strain | |||
| fracture | 800 | % | ASTM D412 |
| tear strength | 15.8 | kN/m | ASTM D624 |
| Compression deformation | |||
| 23℃,24 hr | 11 | % | ASTM D395 |
| THERMAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Embrittlement temperature | < -60.0 | ℃ | ASTM D746 |
| Legal Statement | Nominal value | Unit | Test method |
|---|---|---|---|
| Process Conditions | |||
|---|---|---|---|
| injection | Nominal value | Unit | Test method |
| Squeeze description | Nominal value | Unit | Test method |
| Extrusion | Nominal value | Unit | Test method |
| Barrel rear temperature | 170 to 180 | °C | |
| Barrel middle temperature | 185 to 200 | °C | |
| Barrel front temperature | 185 to 200 | °C | |
| Nozzle temperature | 185 to 200 | °C | |
| Processing (melt) temperature | 185 to 200 | °C | |
| Mold temperature | 10 to 38 | °C | |
| Screw speed | 50 to 100 | rpm | |
| Cushion | 3.56 to 25.4 | mm | |
| Barrel 1 zone temperature | 188 to 204 | °C | |
| Barrel 2 zone temperature | 196 to 207 | °C | |
| Barrel 3 zone temperature | 199 to 210 | °C | |
| Barrel 4 zone temperature | 199 to 210 | °C | |
| Barrel 5 zone temperature | 204 to 216 | °C | |
| Nozzle temperature | 204 to 216 | °C | |
| Notes |
|---|
| 1. Typical properties: these are not to be construed as specifications. |
| 2. Die C, 20 in/min |
| 3. Type 1 |
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |