NGH070IU High Density Polyethylene Resin manufactured by IEPL using “SCLAIRTECH” solution polymerisation process of DU Pont, Canada (Now Nova Chemicals) offers medium molecular weight material with narrow molecular weight distribution to exhibit improved processability, excellent impact strength, stress crack resistance and UV stability for outdoor use at minimum warpage to injection moulded parts like crates, pallets, large containers, Moulded bins etc.&& |
Product Description | |
---|---|
Generic | HDPE |
Material Status | Commercial: Active |
Features | Weather resistance is good,Low warping,Excellent Processability,Good surface appearance,High impact resistance,Good Dimensional Stability,Weight distribution,High ESCR |
Availabilitys | Africa & Middle East ,North America,Asia Pacific,Europe |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.958 | g/cm³ | ASTM D792 |
Melt Flow Rate | |||
190℃,2.16kg | 7.0 | g/10min | ASTM D1238 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Notched impact strength of cantilever beam | 88 | J/m | ASTM D256 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Vicat Softening Temp | 128 | ℃ | ASTM D1525 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Shore hardness | |||
Shaw’s D | 69 | ASTM D2240 | |
tensile strength | |||
yield | 25.0 | MPa | ASTM D638 |
Tensile strain | |||
fracture | 800 | % | ASTM D638 |
Bending modulus | 900 | MPa | ASTM D790 |
bending strength | |||
yield | 30.0 | MPa | ASTM D790 |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |