About |
---|
Fibremod GE277AI is a 20% chemically coupled glass fibre reinforced polypropylene compound intended for injection moulding. This material has an excellent balance between impact strength and stiffness and is easy to process. The product is available in standard black 9502. Applications Fibremod GE277AI has been developed especially for demanding applications in the automotive industry. Structural parts Instrument panel carriers Automotive interior applications Special Features Fibremod GE277AI is suitable for processing with special foaming technologies. Very high flowability&& |
Product Description | |
---|---|
Supplier | Borealis AG |
Generic | Polyolefin Elastomer |
Material Status | Commercial: Active |
Features | High liquidity,Renewable resources |
Availabilitys | Africa & Middle East ,Asia Pacific,Europe |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.04 | g/cm³ | ISO 1183 |
Melt Flow Rate | |||
230℃,2.16kg | 12 | g/10min | ISO 1133 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Tensile modulus | |||
1 mm | 4900 | MPa | ISO 527-2 |
tensile strength | 85.0 | MPa | ISO 527-2 |
Tensile strain | |||
fracture | 3.0 | % | ISO 527-2 |
Bending modulus | 4200 | MPa | ISO 178 |
bending strength | 107 | MPa | ISO 178 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | ||
-20℃ | 9.5 | kJ/m² | ISO 179/1eA |
23℃ | 11 | kJ/m² | ISO 179/1eA |
Charpy Unnotch Impact strength | ISO 179/1eU | ||
-20℃ | 52 | kJ/m² | ISO 179/1eU |
23℃ | 50 | kJ/m² | ISO 179/1eU |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
1.8 MPa, unannealed | 142 | ℃ | ISO 75-2/A |
Vicat Softening Temp | 120 | ℃ | ISO 306/B |
FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
---|---|---|---|
Fogging(100℃) | < 2.0 | mg | DIN 75201 |
Supplementary information | Nominal value | Unit | Test method |
---|---|---|---|
discharge | < 50.0 | µgC/g | VDA 277 |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Mold temperature | 30 to 70 | °C | |
Hold pressure | 30.0 to 70.0 | MPa |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. 0.079 in/min |
3. 16 h |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |