TAROMID A 280 H G9 DX0 TR1

About
Polyamide 66 medium viscosity 45% glass fibres reinforced, flame retardant UL94 V0, heat stabilized, very good flame proofing also at low thickness. Very high mechanical and thermal properties, very low shrinkage and high dimensional stability, high tracking resistance.&&

Product Description
GenericPA66
Material StatusCommercial: Active
FeaturesGood Dimensional Stability,Low contractility,Flame Characteristics,Heat Stabilized,Electric mark,V-0
AvailabilitysEurope
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.61 to 1.63g/cm³ISO 1183
Shrinkage rate Internal Method
TD0.25 to 0.50%Internal Method
MD0.15 to 0.30%Internal Method
Water absorption rate ISO 62
23℃,24hr0.40%ISO 62
Saturation, 23 ℃3.0%ISO 62
Granule Humidity< 0.15%

MECHANICALNominal valueUnitTest method
Tensile modulus12000MPaISO 527-1-2
tensile strength
fracture170MPaISO 527-2/50
Tensile strain
fracture1.5%ISO 527-2/50
Bending modulus11000MPaISO 178
bending strength230MPaISO 178

IMPACTNominal valueUnitTest method
Charpy Notched Impact Strength
23℃8.5kJ/m²ISO 179/1eA
Charpy Unnotch Impact strength
23℃40kJ/m²ISO 179/1eU
Impact strength of cantilever beam notch
23℃85J/mASTM D256

THERMALNominal valueUnitTest method
Hot deformation temperature
1.8 MPa, unannealed244ISO 75-2/A
Continuous use temperature180IEC 60216
Vicat Softening Temp
B50246ISO 306
Ball pressure test
230℃通过 IEC 60695-10-2
Melting temperature250 to 256ISO 11357-3

Electrical performanceNominal valueUnitTest method
Volume resistivity1.0E+15ohms·cmIEC 60093
Dielectric strength
2 mm28kV/mmIEC 60243-1
Dielectric constant3.70 IEC 60250
Compared to the leakage tracing index
Solution A> 400VIEC 60112

FLAME CHARACTERISTICSNominal valueUnitTest method
Flame retardant level UL 94
0.75 mmV-0 UL 94
1.60 mmV-0 UL 94
3.20 mmV-0 UL 94
Glowing wire flammability index
1.0 mm960IEC 60695-2-12
Igniting temperature of the hot wire
1 mm875IEC 60695-2-13
Extreme oxygen index36%ASTM D2863

Supplementary informationNominal valueUnitTest method
Ash Content
850℃45%ISO 3451

Process Conditions
injectionNominal valueUnitTest method
Drying temperature80 to 90°C
Drying time1.0hr
Processing (melt) temperature270 to 300°C
Mold temperature90 to 110°C

Notes
1. Typical properties: these are not to be construed as specifications.
2. TARO 002
3. 0.039 in/min
4. 120°C/hr
5. Short term
6. 1 hr
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.