About |
---|
Sarlink TPE ME-2170 NAT is a general purpose thermoplastic elastomer designed for exterior automotive molding applications. Sarlink TPE ME-2170 NAT is a medium hardness, high density, filled grade having good UV resistance.&& |
Product Description | |
---|---|
Supplier | Teknor Apex |
Generic | TPE |
Material Status | Commercial: Active |
Features | Weather resistance is good,Excellent Processability,Good flexibility,Good liquidity,Good bond,High density,Solvent resistance |
Availabilitys | Africa & Middle East ,North America,Latin America,Asia Pacific,Europe |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.18 | g/cm³ | ASTM D792 |
Melt Flow Rate | |||
200℃,2.16kg | 11 | g/10min | ASTM D1238 |
elastic body | Nominal value | Unit | Test method |
---|---|---|---|
tensile strength | |||
fracture | 6.50 | MPa | ASTM D412 |
Tensile strain | |||
fracture | 700 | % | ASTM D412 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Shore hardness | |||
Shaw’s A | 73 | ASTM D2240 |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Barrel rear temperature | 199 to 210 | °C | |
Barrel middle temperature | 204 to 216 | °C | |
Barrel front temperature | 210 to 221 | °C | |
Nozzle temperature | 216 to 227 | °C | |
Processing (melt) temperature | 216 to 227 | °C | |
Mold temperature | 35 to 66 | °C | |
Injection pressure | 1.38 to 6.89 | MPa | |
Injection speed | Fast | ||
Back pressure | 0.172 to 0.862 | MPa | |
Screw speed | 50 to 120 | rpm | |
Cushion | 3.81 to 25.4 | mm |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |