About |
---|
NORYL GTX GTX964W resin is a blend of Polyphenylene Ether and Polyamide resin with very high impact and high flow. The material wsa designed for large parts, body panels, and thinwall applications. |
Product Description | |
---|---|
Supplier | SABIC |
Generic | PPO(PPE)+PS+PA |
Material Status | Commercial: Active |
Features | High impact resistance,High liquidity |
Availabilitys | North America,Latin America |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.08 | g/cm³ | ASTM D792 |
Melt Volume Rate | |||
280℃,2.16 kg | 7.00 | cm³/10min | ISO 1133 |
Shrinkage rate | |||
MD | 1.5 | % | |
TD | 1.3 | % | |
Water absorption rate | |||
Equilibrium, 23 ℃ | 3.5 | % | |
Balance, 50% RH | 1.2 | % |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Tensile strength | |||
yield | 44.0 | MPa | ASTM D638 |
yield | 50.0 | MPa | ISO 527-2/50 |
fracture | 45.0 | MPa | ISO 527-2/50 |
Tensile strain | |||
yield | 4.0 | % | ISO 527-2/50 |
fracture | 56 | % | ASTM D638 |
fracture | 50 | % | ISO 527-2/50 |
Bending modulus | |||
100 mm span | 1830 | MPa | ASTM D790 |
— | 1800 | MPa | ISO 178 |
Bending stress | |||
— | 70.0 | MPa | ISO 178 |
Yield, 100 mm span | 73.0 | MPa | ASTM D790 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Notched Impact Strength | |||
-30℃ | 20 | kJ/m² | |
23℃ | 45 | kJ/m² | |
Impact strength of cantilever beam notch | |||
23℃ | 530 | J/m | ASTM D256 |
-30℃ | 20 | kJ/m² | ISO 180-1A |
23℃ | 50 | kJ/m² | ISO 180-1A |
Dart impact equipped with measuring instruments (23 ° C, Total Energy) | 41.0 | J | ASTM D3763 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
0.45 MPa, unannealed, 6.4 mm | 185 | ℃ | ASTM D648 |
0.45 MPa, unannealed, 100 mm span | 175 | ℃ | ISO 75-2/Be |
Vicat Softening Temp | |||
— | 240 | ℃ | ISO 306/A50 |
— | 175 | ℃ | ISO 306 |
— | 180 | ℃ | ISO 306/B120 |
Thermal conductivity coefficient | 0.23 | W/m/K | ASTM C177 |
Process Conditions | |||
---|---|---|---|
Injection | Nominal value | Unit | Test method |
drying temperature | 95 to 105 | °C | |
Drying time | 3.0 to 4.0 | hr | |
Recommended maximum moisture content | 0.070 | % | |
Suggested injection volume | 30 to 50 | % | |
Temperature at the rear of the barrel | 275 to 315 | °C | |
Temperature in the middle of the barrel | 280 to 315 | °C | |
Front temperature of material barrel | 290 to 315 | °C | |
Nozzle temperature | 295 to 315 | °C | |
Processing (melt) temperature | 295 to 315 | °C | |
Mold temperature | 75 to 120 | °C | |
Back pressure | 0.300 to 1.40 | MPa | |
Screw speed | 20 to 100 | rpm | |
Exhaust hole depth | 0.013 to 0.038 | mm |
Notes |
---|
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |