Product Description: 65 Shore A TPE for injection molding offering uniform surface appearance, improved abrasion resistance, high flexibility, elasticity/recovery and adhesion (overmolding) to Polypropylene. Features: Overmold/coextrusion adhesion to Polypropylene Rubberlike elasticity low compression set up to 70C Good ozone resistance Good UV resistance Ease of coloring by proper masterbatch&& |
Product Description | |
---|---|
Generic | TPE |
Material Status | Commercial: Active |
Features | Weather resistance is good,Good surface appearance,Good Dimensional Stability,High elastic,High Flexibility,Good bond,Good wear resistance,Ozone resistance,Good coloring |
Availabilitys | North America |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.13 | g/cm³ | ASTM D792 |
Melt Flow Rate | |||
190℃,5.0kg | 9.2 | g/10min | ASTM D1238 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Shore hardness | |||
Shore A, 10 seconds, extrusion molding | 62 | ||
Shore A, 10 seconds, injection molding | 65 |
elastic body | Nominal value | Unit | Test method |
---|---|---|---|
tensile strength | |||
fracture | 5.86 | MPa | ASTM D412 |
100% strain | 1.78 | MPa | ASTM D412 |
Tensile strain | |||
fracture | 610 | % | ASTM D412 |
tear strength | 28.9 | kN/m | ASTM D624 |
Compression deformation | |||
23℃,22 hr | 20 | % | |
70℃,22 hr | 49 | % |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Continuous use temperature | 105 | ℃ | |
Embrittlement temperature | -55.0 | ℃ |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Squeeze description | Nominal value | Unit | Test method |
Extrusion | Nominal value | Unit | Test method |
Drying temperature | 66 to 71 | °C | |
Drying time | 2.0 to 3.0 | hr | |
Barrel rear temperature | 170 to 200 | °C | |
Barrel middle temperature | 180 to 210 | °C | |
Barrel front temperature | 190 to 220 | °C | |
Nozzle temperature | 200 to 230 | °C | |
Processing (melt) temperature | 200 to 220 | °C | |
Mold temperature | 10 to 50 | °C | |
Screw speed | 50 to 200 | rpm | |
Drying temperature | 66 to 71 | °C | |
Drying time | 2.0 to 3.0 | hr | |
Barrel 1 zone temperature | 160 to 180 | °C | |
Barrel 2 zone temperature | 170 to 190 | °C | |
Barrel 3 zone temperature | 180 to 200 | °C | |
Barrel 4 zone temperature | 190 to 210 | °C | |
Melt temperature | 190 to 200 | °C | |
Nozzle temperature | 190 to 210 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |