About |
---|
Visico FR4450/LE4439 is a scorch retardant, moisture-crosslinking polyethylene compound for low voltage insulation. FR4450/LE4439 is a natural, zero halogen, moisture-induced crosslinking polyethylene compound that is designed for use as low voltage wire insulation and jacketing. The combination of a VISICO FR4450 base resin, and the LE4439 catalyst, provides a highly scorch retardant compound with excellent thermal stability and good retardant flame properties. FR4450/LE4439 contains a patented scorch retardant additive (SRA) that increases the processing window for a moisture crosslinking compound and minimizes the tendency for premature crosslinking in the extruder, head or die. A finished compound that is composed of 95 parts of FR4450 mixed with 5 parts of LE4439 is recognized by Underwriters Laboratories as VISICO FR4450/LE4439 95/5. FR4450/LE4439 is designed to reduce normal PE flame spread characteristics and achieve an HB-1 flame rating on 14 AWG wires and larger. LE4439 also provides, in addition to catalyst, a stabilization package containing suitable antioxidants, a metal passivator and a metal deactivator. Properly mixed, during the extrusion process, FR4450/LE4439 exhibits excellent thermal stability to oxidation. FR4450/LE4439 is readily pigmented to a variety of colors using standard wire & cable color concentrates designed for thermoplastic or crosslinked polyethylene. Application FR4450/LE4439 is recommended for use as insulation and sheath for low voltage control cables and power cables up to 6kv in rating. Specifications UL 44&& |
Product Description | |
---|---|
Supplier | Borealis AG |
Generic | PE |
Material Status | Commercial: Active |
Features | Crosslinked,Halogen free,Flame Characteristics,Inoxidizability,Heat Stabilized,Good coloring |
Availabilitys | Africa & Middle East ,North America,Latin America,Asia Pacific,Europe |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | |||
— | 0.940 | g/cm³ | |
— | 1.10 | g/cm³ | |
Melt Flow Rate | |||
190℃,2.16kg | 0.70 | g/10min | ASTM D1238 |
elastic body | Nominal value | Unit | Test method |
---|---|---|---|
tensile strength | MPa | ASTM D412 | |
Tensile strain | |||
fracture | > 300 | % | ASTM D412 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
High temperature creep | |||
Elongation under load: 150 ℃ | < 50 | % | |
Permanent deformation: 150 ℃ | < 5.0 | % |
Electrical performance | Nominal value | Unit | Test method |
---|---|---|---|
Volume resistivity | > 1.0E+16 | ohms·cm | ASTM D257 |
Dielectric strength | > 22 | kV/mm | ASTM D149 |
Dielectric constant | |||
50 Hz | < 3.00 | ASTM D150 | |
Dissipation factor | < 2.0E-3 | ASTM D150 |
FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
---|---|---|---|
Extreme oxygen index | 32 | % | ASTM D2863 |
Corrosive gases in flue gas | 15.0 | µS/cm | IEC 60754-2 |
Supplementary information | Nominal value | Unit | Test method |
---|---|---|---|
Horizontal Flame Test(14 AWG,762.0 µm) | Pass | UL 44 |
Process Conditions | |||
---|---|---|---|
Extrusion | Nominal value | Unit | Test method |
Barrel 1 zone temperature | 140 | °C | |
Barrel 2 zone temperature | 140 | °C | |
Barrel 3 zone temperature | 150 | °C | |
Barrel 4 zone temperature | 160 | °C | |
Barrel 5 zone temperature | 170 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. LE4439 |
3. Visico FR4450 |
4. 0.20 MPa |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |