About |
---|
TECHNYL® C 216 V50 Natural is a polyamide 6, reinforced with 50% of glass fibre, for injection moulding. This grade offers high mechanical strength, good surface aspect for injection moulding.&& |
Product Description | |
---|---|
Supplier | DOMO |
Generic | PA6 |
Material Status | Commercial: Negative |
Features | Good Dimensional Stability,Good Rigidity,Good stripping performance |
Availabilitys | Africa & Middle East ,Europe,Latin America,Asia Pacific,North America |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.56 | g/cm³ | ISO 1183 |
Water absorption rate | |||
23°C,50% RH | 2.2 – 2.4 | % | ISO 62 |
23°C,24 hr | 1.4 – 1.5 | % | ISO 62 |
saturated | 6.2 | % | ISO 62 |
Shrinkage rate | |||
MD | 0.2 – 0.4 | % | ISO 294-4, 2577 |
TD | 0.7 – 0.9 | % | ISO 294-4, 2577 |
Melt Volume Rate | |||
275°C,5kg | 30 | cm³/10min | ISO 1133 |
Viscosity value | |||
96% H2SO4 | 125 | cm³/g | ISO 307 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Tensile modulus | |||
1 mm/min | 16500 | MPa | ISO 527-1/-2 |
Tensile stress | |||
5 mm/min | 230 | MPa | ISO 527-1/-2 |
Tensile strain | |||
5 mm/min | 3 | % | ISO 527-1/-2 |
Bending modulus | |||
2 mm/min | 15000 | MPa | ISO 178 |
bending strength | |||
2 mm/min | 350 | MPa | ISO 178 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy impact strength | |||
23°C | 100 | KJ/m² | ISO 179/1eU |
-30°C | 90 | KJ/m² | ISO 179/1eU |
Charpy Notched Impact Strength | |||
23°C | 20 | kJ/m² | ISO 179/1eA |
-30°C | 15 | kJ/m² | ISO 179/1eA |
Izod notched impact strength | 95 | KJ/m² | ISO 180/1U |
Impact strength of cantilever beam notch | |||
23°C | 19 | KJ/m² | ISO 180/1A |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Melting temperature | 221 | ℃ | ISO 11357-1 |
Hot deformation temperature | |||
0.45 MPa | 220 | ℃ | ISO 75 |
1.80 MPa | 210 | ℃ | ISO 75 |
Vicat Softening Temp | |||
50°C/h – 50N | 215 | ℃ | ISO 306 |
Electrical performance | Nominal value | Unit | Test method |
---|---|---|---|
Volume resistivity | 1E+13 | ohm·cm | IEC 62631-3-1 |
Surface resistivity | 1E+14 | ohm | IEC 62631-3-1 |
FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
---|---|---|---|
Flame retardant level | |||
0.75mm | HB | UL 94 | |
Burning rate | |||
FMVSS,1mm | <100mm/min | FMVSS 302 |
Process Conditions | |||
---|---|---|---|
Injection | Nominal value | Unit | Test method |
drying temperature | 75 – 85 | °C | |
Recommended maximum moisture content | 0.20 | % | |
Temperature at the rear of the barrel | 235 – 240 | °C | |
Temperature in the middle of the barrel | 240 – 250 | °C | |
Front temperature of material barrel | 250 – 260 | °C | |
Mold temperature | 60 – 90 | °C | |
Melt Temperature | 235 – 260 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |