About |
---|
Braskem C7061-01N Polypropylene Resin is a high performance impact copolymer developed for extrusion and blow molding applications. Braskem C7061-01N Polypropylene Resin is a high stiffness, high impact copolymer offering an excellent combination of high stiffness and toughness with excellent processability. Braskem C7061-01N Polypropylene Resin is nucleated and features very high crystallization temperature. Applications for Braskem C7061-01N Polypropylene Resin: Sheet Blow molding Extrusion profiles Thermoforming Complies with: EU, No 10/2011 U.S. FDA FCN 843 Consult the regulations for complete details&& |
Product Description | |
---|---|
Supplier | Braskem |
Generic | PP homopolymerization |
Material Status | Commercial: Active |
Availabilitys | Asia Pacific,Europe |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.900 | g/cm³ | ISO 1183 |
Melt Flow Rate | |||
230℃,2.16kg | 1.5 | g/10min | ISO 1133 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
tensile strength | |||
Yield, injection molding | 27.0 | MPa | ISO 527-2 |
Tensile strain | |||
Yield, injection molding | 7.0 | % | ISO 527-2 |
Bending modulus | |||
injection molding | 1450 | MPa | ISO 178 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Notched Impact Strength | ISO 179/1eA | ||
-20 ℃, injection molding | 8.0 | kJ/m² | |
0 ℃, injection molding | 12 | kJ/m² | |
23 ℃, injection molding | 55 | kJ/m² |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
0.45 MPa, unannealed | 95.0 | ℃ | ISO 75-2/B |
Vicat Softening Temp | 151 | ℃ | ISO 306/A |
Notes |
---|
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |