About |
---|
Graft Resin component for PolyOne’s Syncure™ system, which is a two-step, silane-grafted, moisture-crosslinkable polyethylene system. Graft Resins have approximate shelf life of 6 months from the date of production. Please consult PolyOne for its use past 6 months.&& |
Product Description | |
---|---|
Supplier | Polyone |
Generic | XLPE |
Material Status | Commercial: Active |
Availabilitys | Africa & Middle East ,North America,Asia Pacific,Europe |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.924 | g/cm³ | ASTM D1505 |
Apparent density | 0.50 | g/cm³ | Internal Method |
Melt Flow Rate | |||
190℃,2.16kg | 0.73 | g/10min | ASTM D1238 |
Gel content | 75 | % | ASTM D2765 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Tensile modulus | 11.0 | MPa | ASTM D638 |
tensile strength | |||
fracture | 16.5 | MPa | ASTM D638 |
Tensile strain | |||
fracture | 600 | % | ASTM D638 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
deformation | |||
131℃ | 5.7 | % | UL 1581 |
Thermal creep elongation | 45 | % |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Drying temperature | 71 | °C | |
Drying time | 3.0 to 4.0 | hr | |
Barrel rear temperature | 204 to 216 | °C | |
Barrel middle temperature | 171 to 204 | °C | |
Barrel front temperature | 177 to 204 | °C | |
Nozzle temperature | 177 to 216 | °C | |
Mold temperature | 27 to 66 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. Geon® 1169 |
3. Procedure A |
4. Crosslinked PE, Method B (NonReferee Test) |
5. Type IV, 20 in/min |
6. 500 g, 1hr |
7. SYV-40 |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |