VICTREX™ PEEK 450FC30

About
High performance thermoplastic material, 30% reinforced with carbon fibre / graphite / PTFE PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, FDA food contact compliant, colour black. Tribological applications for high strength. Excellent wear resistance, very low coefficient of friction, low coefficient of thermal expansion. Chemically resistant to aggressive environments.&&

Product Description
SupplierVictrex
Material StatusCommercial: Active
FeaturesGood liquidity,Food contact compliance,Hypocrystalline,Low coefficient of friction,Solvent resistance,Good Rigidity,Good wear resistance
AvailabilitysAsia Pacific,North America,Europe,Africa & Middle East ,Latin America
Process MethodsExtrusion,Injection Molding

Technical Data
MECHANICALNominal valueUnitTest method
Shore hardness
Shore D, 23 ℃83 ISO 868
Tensile modulus
23℃13000MPaISO 527-2
tensile strength ISO 527-2
Fracture, 23 ℃150MPaISO 527-2
Fracture, 125 ℃95.0MPaISO 527-2
Fracture, 175 ℃55.0MPaISO 527-2
Fracture, 225 ℃45.0MPaISO 527-2
Fracture, 275 ℃35.0MPaISO 527-2
Tensile strain
Fracture, 23 ℃2.3%ISO 527-2
Bending modulus
23℃11500MPaISO 178
bending strength ISO 178
23℃230MPaISO 178
125℃160MPaISO 178
175℃80.0MPaISO 178
275℃45.0MPaISO 178
compressive strength ISO 604
23℃170MPaISO 604
120℃110MPaISO 604
200℃45.0MPaISO 604

IMPACTNominal valueUnitTest method
Charpy Notched Impact Strength
23℃5.0kJ/m²ISO 179/1eA
Charpy Unnotch Impact strength
23℃35kJ/m²ISO 179/1U
Impact strength of cantilever beam notch
23℃7.0kJ/m²ISO 180-A
Notched impact strength of cantilever beam
23℃35kJ/m²ISO 180

THERMALNominal valueUnitTest method
Hot deformation temperature
1.8 MPa, unannealed315ISO 75-2/Af
Glass transition temperature ISO 11357-2
143ISO 11357-2
150ISO 11357-2
Melting temperature343ISO 11357-3
Linear coefficient of thermal expansion
TD ISO 11359-2
MD ISO 11359-2
< 143℃1.5E-5cm/cm/℃ISO 11359-2
> 143℃2.0E-5cm/cm/℃ISO 11359-2
< 143℃4.5E-5cm/cm/℃ISO 11359-2
> 143℃1.2E-4cm/cm/℃ISO 11359-2
Thermal conductivity coefficient ISO 22007-4
23℃0.85W/m/KISO 22007-4
23℃1.7W/m/KISO 22007-4
Relative temperature index
Strength mechanical performance240UL 746
Impact mechanical performance180UL 746

Electrical performanceNominal valueUnitTest method
Volume resistivity
23℃1.0E+10ohms·cmIEC 60093

FLAME CHARACTERISTICSNominal valueUnitTest method
Glowing wire flammability index
2.0 mm960IEC 60695-2-12
Extreme oxygen index43%ISO 4589-2

PHYSICALNominal valueUnitTest method
Density1.45g/cm³ISO 1183
Spiral flow length Internal Method
8.00cmInternal Method
38.0cmInternal Method
Shrinkage rate ISO 294-4
TD0.70%ISO 294-4
MD0.30%ISO 294-4
Water absorption rate
Saturation, 23 ℃0.35%ISO 62
Saturation, 100 ℃0.45%ISO 62
Apparent viscosity of melt
400℃550Pa·sISO 11443

Process Conditions
injectionNominal valueUnitTest method
Drying temperature120 to 150°C
Drying time3.0 to 5.0hr
Hopper temperature< 100°C
Barrel rear temperature365°C
Barrel middle temperature370 to 375°C
Barrel front temperature380°C
Nozzle temperature385°C
Mold temperature170 to 200°C

Notes
1. Typical properties: these are not to be construed as specifications.
2. Crystalline
3. Mold Temperature: 392°F, Melt Temperature: 725°F
4. 1 mm
5. 3 mm
6. 385°C nozzle, 200°C tool
7. Onset
8. Midpoint
9. Average
10. Along flow
11. 1V
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.