Iupilon® EGN2030KR is a Polycarbonate (PC) material filled with 30% glass fiber. It is available in Asia Pacific, Europe, or North America for injection molding. Important attributes of Iupilon® EGN2030KR are: Flame Rated Flame Retardant Halogen Free High Flow&& |
Product Description | |
---|---|
Supplier | Mitsubishi |
Generic | Polycarbonate |
Material Status | Commercial: Active |
Features | High liquidity,Halogen free,Flame Characteristics,Low to no phosphorus content,V-2,V-0 |
Availabilitys | North America,Asia Pacific,Europe |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 1.43 | g/cm³ | ISO 1183 |
Shrinkage rate | |||
TD:3.2 mm | 0.20 to 0.40 | % | |
MD:3.2 mm | 0.10 to 0.30 | % | |
Water absorption rate | |||
Saturation, 23 ℃ | 0.090 | % | ISO 62 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
tensile strength | |||
fracture | 100 | MPa | ISO 527-2 |
Tensile strain | |||
fracture | 2.3 | % | ISO 527-2 |
Bending modulus | 8000 | MPa | ISO 178 |
bending strength | 153 | MPa | ISO 178 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Notched Impact Strength | |||
23℃ | 9.0 | kJ/m² | ISO 179 |
Charpy Unnotch Impact strength | |||
23℃ | 32 | kJ/m² | ISO 179 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
1.8 MPa, unannealed | 140 | ℃ | ISO 75-2/A |
0.45 MPa, unannealed | 144 | ℃ | ISO 75-2/B |
Electrical performance | Nominal value | Unit | Test method |
---|---|---|---|
Compared to the leakage tracing index | PLC 3 | UL 746 |
FLAME CHARACTERISTICS | Nominal value | Unit | Test method |
---|---|---|---|
Flame retardant level | UL 94 | ||
0.75 mm | V-2 | UL 94 | |
1.50 mm | V-0 | UL 94 |
Process Conditions | |||
---|---|---|---|
injection | Nominal value | Unit | Test method |
Drying temperature | 120 | °C | |
Drying time | 4.0 to 8.0 | hr | |
Barrel rear temperature | 270 to 290 | °C | |
Barrel middle temperature | 280 to 300 | °C | |
Barrel front temperature | 280 to 300 | °C | |
Nozzle temperature | 280 to 300 | °C | |
Mold temperature | 80 to 120 | °C | |
Injection pressure | 50.0 to 150 | MPa | |
Screw speed | 50 to 100 | rpm |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |