About |
---|
Purell PE GF 4760 is a high density polyethylene with good ESCR, high rigidity and good organoleptic properties. It contains antioxidants and is delivered in pellet form. Target applications are small blow mouldings for foodstuff, consumer goods as well as pharmaceutical packaging. This grade is also well established for injection blow moulding applications. Without exception, all potential activities for applications in the pharmaceutical, medical device, laboratory and diagnostics area have to be discussed with the relevant Technical (P & AD) and Business contacts first. To discuss a medical/pharmaceutical application please contact: your local Distributor or your local Basell contact.&& |
Product Description | |
---|---|
Supplier | LyondellBasell |
Generic | HDPE |
Material Status | Commercial: Active |
Features | Ethylene oxide disinfection,Good liquidity,Inoxidizability,Good Rigidity,High ESCR,Good sensory characteristics. |
Availabilitys | Latin America,Europe,North America,Asia Pacific,Africa & Middle East |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.956 | g/cm³ | ISO 1183 |
Apparent density | > 0.50 | g/cm³ | ISO 60 |
Melt Flow Rate | ISO 1133 | ||
190℃,2.16kg | 0.40 | g/10min | ISO 1133 |
190℃,21.6kg | 30 | g/10min | ISO 1133 |
190℃,5.0kg | 1.5 | g/10min | ISO 1133 |
Basell Bottle Test | 1.3 | day | Internal Method |
Full notch creep test | ISO 16770 | ||
80℃ | 5.0 | hr | ISO 16770 |
80℃ | 15.0 | hr | ISO 16770 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Charpy Notched Impact Strength | |||
-30℃ | 8.0 | kJ/m² | ISO 179/1A |
Tensile Impact Strength | 90.0 | kJ/m² | ISO 8256 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Vicat Softening Temperature | |||
B50 | 77.0 | ℃ | ISO 306 |
Supplementary Information | Nominal value | Unit | Test method |
---|---|---|---|
Stauddinger index | |||
Jg | 280 | cm³/g | ISO 1628 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Shore hardness | |||
Shore D | 62 | ISO 868 | |
Tensile Modulus | 1250 | MPa | ISO 527-2 |
Tensile Strength | |||
27.0 | MPa | ISO 527-2 | |
Tensile Strain | |||
10 | % | ISO 527-2 | |
Ball indentation hardness | |||
H 132/30 | 51.0 | MPa | ISO 2039-1 |
Process Conditions | |||
---|---|---|---|
Extrusion Molded | Nominal value | Unit | Test method |
Melt Temperature | 180 to 220 | °C |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. 3.5 MPa, 2% Arcopal |
3. 2.5 MPa, 2% Arcopal |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |