VALOX™ V4860HR resin

About
VALOX™   V4860HR resin 30% glass reinforced PBT, UL94 V-0 rated, Hydrolytically stable, Impact Modified.&&

Product Description
SupplierSABIC
Genericpolybutylene terephthalate
Material StatusCommercial: Active
FeaturesHigh impact resistance,Hydrolysis stability,V-0
AvailabilitysNorth America,Asia Pacific,Europe
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.64g/cm³ASTM D792
Density1.64g/cm³ISO 1183
Melt Flow Rate
250℃,5.0kg18g/10minASTM D1238
Melt Volume Rate
250℃,5 kg12.4cm³/10minISO 1133
Shrinkage rate
TD:3.2 mm0.50 to 1.0%Internal Method
MD:3.2 mm0.50 to 0.70%Internal Method
Water absorption rate
Saturation, 23 ℃0.19%ISO 62
Equilibrium, 23 ℃, 50% RH0.060%ISO 62

MECHANICALNominal valueUnitTest method
Tensile modulus9750MPaASTM D638
Tensile modulus9450MPaISO 527-1-2
tensile strength
fracture111MPaISO 527-2/5
fracture115MPaASTM D638
yield116MPaASTM D638
yield112MPaISO 527-2/5
Tensile strain
fracture2.2%ISO 527-2/5
fracture2.3%ASTM D638
yield2.3%ASTM D638
yield2.1%ISO 527-2/5
Bending modulus7880MPaISO 178
50 mm span6740MPaASTM D790
bending strength ISO 178
Fracture, 50 mm span2.96MPaASTM D790
Yield, 50 mm span174MPaASTM D790
182MPaISO 178
183MPaISO 178
Fracture bending strain2.9%ISO 178

IMPACTNominal valueUnitTest method
Charpy Notched Impact Strength
23℃11kJ/m²ISO 179/1eA
Impact strength of cantilever beam notch ASTM D256
-30℃74J/mASTM D256
23℃90J/mASTM D256
Impact strength of cantilever beam notch ISO 180/1A
-30℃8.5kJ/m²ISO 180-1A
23℃10kJ/m²ISO 180-1A
Dart impact equipped with measuring instruments
23℃,Total Energy13.4JASTM D3763

THERMALNominal valueUnitTest method
Hot deformation temperature ASTM D648
1.8 MPa, unannealed, 64 mm span188ISO 75-2/Af
0.45 MPa, unannealed, 6.4 mm221ASTM D648
1.8 MPa, unannealed, 3.2 mm197ASTM D648
1.8 MPa, unannealed, 6.4 mm205ASTM D648
Vicat Softening Temp176ASTM D1525 12
Vicat Softening Temp 
B50176ISO 306
B120175ISO 306/B120
Ball pressure test
75℃Pass IEC 60695-10-2
Linear coefficient of thermal expansion
TD:23~80℃1.2E-41/℃ISO 11359-2
TD:-40~95℃1.1E-41/℃ASTM E831
MD:23~80℃2.3E-51/℃ISO 11359-2
MD:-40~95℃2.4E-51/℃ASTM E831

FLAME CHARACTERISTICSNominal valueUnitTest method
0.80 mmV-0 UL 94

Process Conditions
injectionNominal valueUnitTest method
Drying temperature120°C
Drying time3.0 to 4.0hr
Drying time, maximum12hr
Recommended maximum moisture content0.020%
Recommended injection volume30 to 70%
Barrel rear temperature220 to 240°C
Barrel middle temperature230 to 250°C
Barrel front temperature240 to 260°C
Nozzle temperature240 to 260°C
Processing (melt) temperature230 to 260°C
Mold temperature60 to 120°C
Back pressure0.345 to 0.690MPa
Screw speed20 to 100rpm
Vent depth0.025 to 0.038mm

Notes
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.