Multilon® TN-7000A

About

Product Description
SupplierTEIJIN
GenericPC+ABS
Material StatusCommercial: Negative
FeaturesFlame Characteristics,V-2,5VB,Halogen free,V-1,V-0
AvailabilitysAfrica & Middle East ,North America,Latin America,Asia Pacific,Europe
Process MethodsInjection Molding

Technical Data
PHYSICALNominal valueUnitTest method
Density1.18g/cm³ISO 1183
Molding shrinkage Internal Method
TD:4.0 mm0.50 to 0.70%Internal Method
MD:4.0 mm0.50 to 0.70%Internal Method

MECHANICALNominal valueUnitTest method
Tensile Strength
Broken BRK53.0MPaISO 527-2/50
Yield yld65.0MPaISO 527-2/50
Tensile Strain
Broken BRK120%ISO 527-2/50
Flexural Modulus2600MPaISO 178
Flexural Strength95.0MPaISO 178

IMPACTNominal valueUnitTest method
Charpy Notched Impact Strength35kJ/m²ISO 179

THERMALNominal valueUnitTest method
Hot deformation temperature HDT
1.8 MPa, unannealed84.0ISO 75-2/A
0.45 MPa, unannealed94.0ISO 75-2/B
Vicat Softening Temperature
B5097.0ISO 306
Coeff. of linear thermal expansion
TD8.0E-51/℃ISO 11359-2
MD8.0E-51/℃ISO 11359-2
Relative Temperature Index (RTI)
Electrical Elec85UL-746B
Impact85UL-746B
Strength Str85UL-746B

ELECTRICALNominal valueUnitTest method
Surface Resistivity1.0E+16ohmsIEC 60093
Compared Tracking Index2PLC CodeUL 746
High Arc Burning Index (HAI)
1.2 mm3 PLC CodeUL 746A
1.5 mm3 PLC CodeUL 746A
2.0 mm2 PLC CodeUL 746A
3.0 mm2 PLC CodeUL 746A
Hot wire ignition
1.2 mm3PLC CodeUL 746A
1.5 mm3PLC CodeUL 746A
2.0 mm2PLC CodeUL 746A
3.0 mm2PLC CodeUL 746A

FLAME CHARACTERISTICSNominal valueUnitTest method
Flame Class Rating UL 94
0.70 mmV-2 UL 94
1.20 mmV-1 UL 94
1.50 mmV-0 UL 94
2.00 mm5VB UL 94

Process Conditions
Injection MoldingNominal valueUnitTest method
Drying Temperature80
Drying Time5-8hr
Melt Temperature230
Mold Temperature270

Notes
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.