Akulon® F136-C1

About
Very High Viscosity, Film Extrusion, Lubricated&&

Product Description
SupplierDSM
GenericPA6
Material StatusCommercial: Active
FeaturesUltra High Viscosity,Lubricating
AvailabilitysAsia Pacific,Europe
Process MethodsFilm extrusion

Technical Data
MECHANICALNominal valueUnitTest method
friction coefficient ISO 8295
With oneself – dynamic, casting thin films1.0 ISO 8295
Compared to itself – static, cast thin films1.2 ISO 8295

filmNominal valueUnitTest method
film thickness
test50µm
Tensile modulus
50 µ m, cast thin film450MPaInternal Method
tensile strength
MD, yield, 50 µ m, blow molded film31.0MPaISO 527-3
MD, 50 µ m, blow molded film83.0MPaISO 527-3
Tensile strain
MD, fracture, 50 µ m, cast thin film350%ISO 527-3
Pant tear resistance
MD, 50 µ m, cast thin film32.0N/mmISO 6383-1
Water vapor transmittance
23 ℃, 85% RH, 50 µ m, cast thin film35g/m²/24 hrDIS 15106-1/-3
Oxygen transfer rate DIS 15105-1/-2
0% RH:23℃,50.0 µm27cm³/m²/bar/24 hrDIS 15105-1/-2
85% RH:23℃,50.0 µm39cm³/m²/bar/24 hrDIS 15105-1/-2

THERMALNominal valueUnitTest method
Linear coefficient of thermal expansion
MD9.0E-51/℃ISO 11359-2
Specific heat capacity 
1550J/kg/℃
Average: 20 to 150 ℃2250J/kg/℃

optical performanceNominal valueUnitTest method
Transmittance
50.0 µ m, cast thin film83.0%Internal Method

Supplementary informationNominal valueUnitTest method
Puncture resistance
50.0 µm14.0J/cmInternal Method
RSV3.60 Internal Method

PHYSICALNominal valueUnitTest method
Density1.13g/cm³ISO 1183
Viscosity number245cm³/gISO 307
Apparent viscosity of melt
260℃2250Pa·sInternal Method

Process Conditions
injectionNominal valueUnitTest method
ExtrusionNominal valueUnitTest method
Drying temperature80°C
Drying time4.0 to 8.0hr
Barrel rear temperature230 to 235°C
Barrel middle temperature235 to 250°C
Barrel front temperature240 to 260°C
Nozzle temperature240 to 270°C
Processing (melt) temperature240 to 275°C
Mold temperature50 to 80°C
Injection speedModerate-Fast 
Back pressure3.00 to 10.0MPa
Screw compression ratio2.5:1.0 
Drying temperature75°C
Drying time8.0 to 10hr
Barrel 1 zone temperature240°C
Barrel 2 zone temperature260°C
Barrel 3 zone temperature260°C
Connector temperature270°C
Nozzle temperature260°C

Notes
1. Typical properties: these are not to be construed as specifications.
2. 2.0 in/min
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.