| About |
|---|
| ADIPRENE L 325 is a polyether-based, TDI terminated liquid urethane prepolymer that is readily processable by conventional hand and machine mixing techniques. When cured with 4,4′-methylene-bis(2-chloroaniline), this member of the ADIPRENE L family produces high quality vulcanizates in the 70-75 Shore D hardness range. These tough, highly resilient elastomers have many unique features: Excellent low-temperature flexibility Excellent abrasion resistance Good hydrolytic stability Low compression set ADIPRENE L 325 gives a longer working life when mixed with curatives than does ADIPRENE L 315, so it is more suitable for the preparation of large parts.&& |
| Product Description | |
|---|---|
| Supplier | Chemtura |
| Generic | PUR-脂肪族+TDI |
| Material Status | Commercial: Active |
| Features | Good flexibility,Good Dimensional Stability,Hydrolysis stability,Elastic,Low temperature toughness,Good wear resistance |
| Availabilitys | Asia Pacific |
| Process Methods | casting |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 1.20 | g/cm³ | ASTM D792 |
| elastic body | Nominal value | Unit | Test method |
|---|---|---|---|
| tensile strength | 60.7 | MPa | ASTM D412 |
| 100% strain | 25.9 | MPa | ASTM D412 |
| Tensile strain | |||
| fracture | 260 | % | ASTM D412 |
| tear strength | |||
| cracking | 20 | kN/m | ASTM D470 |
| Compression deformation | |||
| 70℃,22 hr | 10 | % | ASTM D395A |
| Basho’s elasticity | 58 | % | ASTM D2632 |
| IMPACT | Nominal value | Unit | Test method |
|---|---|---|---|
| Impact strength of cantilever beam notch | 640 | J/m | ASTM D256 |
| Supplementary information | Nominal value | Unit | Test method |
|---|---|---|---|
| friction coefficient | |||
| NBS | 425 |
| Uncured Properties | Nominal value | Unit | Test method |
|---|---|---|---|
| Curing time | |||
| 100℃ | 1.0 | hr |
| MECHANICAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Shore hardness | |||
| Shaw’s D | 72 | ASTM D2240 | |
| Bending modulus | 586 | MPa | ASTM D790 |
| THERMAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Embrittlement temperature | < -70.0 | ℃ | ASTM D746 |
| Hot deformation temperature | 145 | ℃ | |
| Thermosetting components | |||
| resin | 按重量计算的混合比: 100 | ||
| Hardening method | 按重量计算的混合比: 90 | ||
| storage stability | 2.5 | min | |
| Post curing time | |||
| 100℃ | 16 | hr |
| Notes |
|---|
| 1. Typical properties: these are not to be construed as specifications. |
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |