About |
---|
ADVANCENE™ EM-4810-AAH HDPE Resin is a polymer with broad molecular weight distribution and high molecular weight. This product provides an excellent combination of extrudability and parison stability, which contribute to uniform wall thickness in large parts. ADVANCENE™ EM-4810-AAH HDPE Resin is ideal for blow molding containers of > 80 liters closed head shipping containers and other similar pans. The broad distribution also provides outstanding environmental stress crack resistance (ESCR) at a good rigidity. Because of these characteristics, a wide variety of products, such as industrial chemicals, latex paints, printing inks, foodstuffs, adhesives and other chemical specialties may be packaged in containers produced from this resin. The smooth surface of molded parts is readily treated and printed for high quality applications. Main Characteristics: Outstanding environmental stress crack resistance. Excellent parison melt strength/low sag. Good extrudability/processability. Good rigidty.&& |
Product Description | |
---|---|
Generic | HMW-HDPE |
Material Status | Commercial: Active |
Features | Good Rigidity,Excellent Processability,Wide molecular weight distribution,Good Printability,High molecular weight,High density,High ESCR |
Availabilitys | Africa & Middle East ,Europe |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.948 | g/cm³ | ASTM D792 |
Melt Flow Rate | |||
190℃,21.6kg | 10 | g/10min | ASTM D1238 |
ESCR(Environmental Stress Cracking Resistance) | |||
50 ℃, 100% non-ionic surfactant, F50 | > 1500 | hr | ASTM D1693 |
IMPACT | Nominal value | Unit | Test method |
---|---|---|---|
Tensile impact strength | |||
— | 462 | kJ/m² | ASTM D1822 |
— | 462 | kJ/m² | ISO 8256 |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Hot deformation temperature | |||
0.45 MPa, unannealed | 66.0 | ℃ | ASTM D648 |
Embrittlement temperature | < -76.0 | ℃ | ASTM D746 |
Vicat Softening Temp | 127 | ℃ | ASTM D1525 |
Melting peak temperature | 130 | ℃ | ASTM D3418 |
Crystallization peak temperature | |||
DSC | 114 | ℃ | ASTM D3418 |
MECHANICAL | Nominal value | Unit | Test method |
---|---|---|---|
Shore hardness | |||
Shaw’s D | 57 | ASTM D2240 | |
tensile strength | |||
yield | 22.8 | MPa | |
fracture | 36.5 | MPa | |
Tensile strain | |||
yield | 6.0 | % | |
fracture | 900 | % | |
Bending modulus | |||
2% secant | 855 | MPa | ASTM D790-B |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. Type S |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |