AFFINITY™ PL 1280G Polyolefin Plastomer is a Polyolefin Plastomer (POP) produced using INSITE™ Technology from Dow Plastics. It is specifically designed for use as a sealant layer in flexible structures for the packaging of meat and cheese, dry foods and consumer goods. Due to its excellent sealability at low temperatures, ultimate hot tack strength, optical properties and abuse resistance, it is particularly suitable for high speed form-fill-seal packaging machines. Applications: Cast Film Complies with: Canadian HPFP No Objection EU, No 10/2011 U.S. FDA FCN 424 Consult the regulations for complete details.&& |
Product Description | |
---|---|
Supplier | DOW |
Generic | POP |
Material Status | Commercial: Active |
Availabilitys | North America,Asia Pacific,Europe |
Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.900 | g/cm³ | ASTM D792 |
Melt Flow Rate | |||
190℃,2.16kg | 6.0 | g/10min | ISO 1133 |
film | Nominal value | Unit | Test method |
---|---|---|---|
film thickness | |||
test | 25 | µm | |
tensile strength | ISO 527-3 | ||
MD, yield, 25 µ m | 5.80 | MPa | ISO 527-3 |
TD, yield, 25 µ m | 5.30 | MPa | ISO 527-3 |
MD, fracture, 23 µ m | 48.0 | MPa | ISO 527-3 |
TD, fracture, 23 µ m | 30.0 | MPa | ISO 527-3 |
Tensile strain | ISO 527-3 | ||
MD, fracture, 25 µ m | 470 | % | ISO 527-3 |
TD, fracture, 25 µ m | 720 | % | ISO 527-3 |
Drop hammer impact | |||
25 µm | 290 | g | ISO 7765-1/B |
Elmandorf tear strength | ASTM D1922 | ||
MD:25 µm | 78 | g | ASTM D1922 |
TD:25 µm | 410 | g | ASTM D1922 |
Initial sealing temperature | |||
25 µm | 88.0 | ℃ | Internal Method |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Vicat Softening Temp | 81.0 | ℃ | ASTM D1525 |
Melting temperature | |||
DSC | 96.0 | ℃ | Internal Method |
optical performance | Nominal value | Unit | Test method |
---|---|---|---|
gloss | |||
20°,25 µm | 91 | ASTM D2457 | |
Haze | |||
25 µm | 4.0 | % | ISO 14782 |
Notes |
---|
1. Typical properties: these are not to be construed as specifications. |
2. Single layer cast film, extruded at 274°C, 0.5 mm die gap. |
3. Single layer cast film, extruded at 274°C, 0.5 mm die gap. Temperature required to reach 5.25 N/15 mm heat-seal strength. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |