| About |
|---|
| AMPLIFY™ IO 3801B Ethylene Acrylic Acid Ionomer is designed for blown and cast film coextrusion for flexible packaging applications. It provides excellent sealability in coextrusions with nylon and other film structures with low blocking. For Food and Specialty Applications Excellent sealant for use in blown and cast film coextrusions Complies with: U.S. FDA 21 CFR 177.1310(b) Consult the regulations for complete details.&& |
| Product Description | |
|---|---|
| Supplier | DOW |
| Generic | 离聚物 |
| Material Status | Commercial: Active |
| Availabilitys | North America,Latin America |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 0.940 | g/cm³ | ASTM D792 |
| Melt Flow Rate | |||
| 190℃,2.16kg | 1.3 | g/10min | ASTM D1238 |
| Ionic type | 钠 (Na | ||
| film | Nominal value | Unit | Test method |
|---|---|---|---|
| film thickness | |||
| test | 51 | µm | |
| tensile strength | ASTM D882 | ||
| MD, yield, 51 µ m | 15.2 | MPa | ASTM D882 |
| TD, yield, 51 µ m | 12.5 | MPa | ASTM D882 |
| MD, fracture, 51 µ m | 33.6 | MPa | ASTM D882 |
| TD, fracture, 51 µ m | 34.3 | MPa | ASTM D882 |
| Tensile strain | ASTM D882 | ||
| MD, fracture, 51 µ m | 280 | % | ASTM D882 |
| TD, fracture, 51 µ m | 400 | % | ASTM D882 |
| THERMAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Melting temperature | |||
| DSC | 95.0 | ℃ | Internal Method |
| Notes |
|---|
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |