| About |
|---|
| Andur 9000-AS is a two-component liquid urethane system which can be processed at room temperature to yield an eastomer with a hardness of 90 to 92 Shore A. Andur 9000-AS is recommended where ease of processing is desired.&& |
| Product Description | |
|---|---|
| Generic | PUR+TDI |
| Material Status | Commercial: Active |
| Availabilitys | North America |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 1.08 | g/cm³ | ASTM D792 |
| MECHANICAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Shore hardness | |||
| Shaw’s A | 91 | ASTM D2240 |
| elastic body | Nominal value | Unit | Test method |
|---|---|---|---|
| tensile strength | ASTM D412 | ||
| yield | 24.1 | MPa | ASTM D412 |
| 100% strain | 8.27 | MPa | ASTM D412 |
| 300% strain | 13.8 | MPa | ASTM D412 |
| Tensile strain | |||
| fracture | 300 | % | ASTM D412 |
| Compression deformation | 26 | % | ASTM D395 |
| THERMAL | Nominal value | Unit | Test method |
|---|---|---|---|
| storage stability | 5.0 to 6.0 | min |
| Thermosetting mixed viscosity | Nominal value | Unit | Test method |
|---|---|---|---|
| 25℃ | 700 | cP | ASTM D2393 |
| stripping time | |||
| 22℃ | 2.0 | min | |
| Post curing time | |||
| 100℃ | 6.0 | hr |
| Notes |
|---|
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |