| About |
|---|
| Andur 9500 AP/Curene® 442是一种聚氨酯(聚醚,TDI)(PUR-脂肪族/TDI)产品,。 它,在北美洲有供货。&& |
| Product Description | |
|---|---|
| Generic | PUR-脂肪族+TDI |
| Material Status | Commercial: Active |
| Availabilitys | North America |
| Technical Data | |||
|---|---|---|---|
| PHYSICAL | Nominal value | Unit | Test method |
| Density | 1.14 | g/cm³ | ASTM D1505 |
| Shrinkage rate | |||
| MD | 1.3 | % | ASTM D955 |
| elastic body | Nominal value | Unit | Test method |
|---|---|---|---|
| tensile strength | ASTM D412 | ||
| yield | 31.1 | MPa | ASTM D412 |
| 100% strain | 11.8 | MPa | ASTM D412 |
| 300% strain | 24.5 | MPa | ASTM D412 |
| Tensile strain | |||
| fracture | 340 | % | ASTM D412 |
| Compression deformation | 29 | % | ASTM D395B |
| Basho’s elasticity | 37 | % | ASTM D2632 |
| THERMAL | Nominal value | Unit | Test method |
|---|---|---|---|
| storage stability | 2.0 to 4.0 | min | |
| stripping time | 20 to 30 | min | |
| Post curing time | |||
| 96℃ | 16 | hr |
| MECHANICAL | Nominal value | Unit | Test method |
|---|---|---|---|
| Shore hardness | |||
| Shaw’s A | 95 | ASTM D2240 | |
| compressive strength | ASTM D695 | ||
| 5% strain | 0.945 | MPa | ASTM D695 |
| 10% strain | 3.61 | MPa | ASTM D695 |
| 15% strain | 5.95 | MPa | ASTM D695 |
| 25% strain | 9.12 | MPa | ASTM D695 |
| Process Conditions | |||
|---|---|---|---|
| injection | Nominal value | Unit | Test method |
| Mold temperature | 104 to 113 | °C | |
| Notes |
|---|
| 【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |