Technical Data | |||
---|---|---|---|
PHYSICAL | Nominal value | Unit | Test method |
Density | 0.904 | g/cm³ | ASTM D792 |
Melt Flow Rate | |||
190℃,2.16kg | 4.0 | g/10min | ASTM D1238 |
film | Nominal value | Unit | Test method |
---|---|---|---|
Membrane puncture resistance | Internal Method | ||
20 µm | 18.9 | J/cm³ | Internal Method |
51 µm | 17.5 | J/cm³ | Internal Method |
Secant modulus | ASTM D882 | ||
2% secant, MD: 20 µ m | 58.8 | MPa | ASTM D882 |
2% secant, MD: 51 µ m | 62.6 | MPa | ASTM D882 |
2% secant, TD: 20 µ m | 64.7 | MPa | ASTM D882 |
2% secant, TD: 51 µ m | 63.0 | MPa | ASTM D882 |
tensile strength | ASTM D882 | ||
MD, yield, 20 µ m | 7.00 | MPa | ASTM D882 |
MD, yield, 51 µ m | 6.76 | MPa | ASTM D882 |
TD, yield, 20 µ m | 4.92 | MPa | ASTM D882 |
TD, yield, 51 µ m | 6.34 | MPa | ASTM D882 |
MD, fracture, 20 µ m | 36.9 | MPa | ASTM D882 |
MD, fracture, 51 µ m | 32.6 | MPa | ASTM D882 |
TD, fracture, 20 µ m | 29.1 | MPa | ASTM D882 |
TD, fracture, 51 µ m | 32.4 | MPa | ASTM D882 |
Tensile strain | ASTM D882 | ||
MD, fracture, 20 µ m | 500 | % | ASTM D882 |
MD, fracture, 51 µ m | 660 | % | ASTM D882 |
TD, fracture, 20 µ m | 710 | % | ASTM D882 |
TD, fracture, 51 µ m | 710 | % | ASTM D882 |
Drop hammer impact | ASTM D1709B | ||
20 µm | > 850 | g | ASTM D1709-B |
51 µm | > 850 | g | ASTM D1709-B |
Elmandorf tear strength | ASTM D1922 | ||
MD:20 µm | 330 | g | ASTM D1922 |
MD:51 µm | 960 | g | ASTM D1922 |
TD:20 µm | 500 | g | ASTM D1922 |
TD:51 µm | 1100 | g | ASTM D1922 |
Oxygen permeability | |||
23℃,51 µm | 450 | cm³·mm/m²/atm/24 hr | ASTM D3985 |
Water vapor transmittance | |||
51 µm | 0.85 | g·mm/m²/atm/24 hr | ASTM F1249 |
Carbon dioxide transfer rate | |||
23℃,50.8 µm | 2000 | cm³·mm/m²/atm/24 hr | Internal Method |
THERMAL | Nominal value | Unit | Test method |
---|---|---|---|
Vicat Softening Temp | 71.1 | ℃ | ASTM D1525 |
Melting temperature | |||
DSC | 124 | ℃ | Internal Method |
optical performance | Nominal value | Unit | Test method |
---|---|---|---|
gloss | ASTM D2457 | ||
45°,20.3 µm | 92 | ASTM D2457 | |
45°,50.8 µm | 90 | ASTM D2457 | |
transparency | ASTM D1746 | ||
20.3 µm | 99.0 | ASTM D1746 | |
50.8 µm | 99.0 | ASTM D1746 | |
Haze | ASTM D1003 | ||
20.3 µm | 0.60 | % | ASTM D1003 |
50.8 µm | 1.8 | % | ASTM D1003 |
Notes |
---|
1. Conditions of Use A through H |
2. With limitations |
3. Typical properties: these are not to be construed as specifications. |
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |