AvaSpire® AV-630

About
AvaSpire® AV-630 is an unreinforced polyaryletherketone (PAEK) developed as an alternative to low melt flow PEEK for the extrusion of ultra-thin films. Films with thicknesses as low as 0.2 mils (5 microns) can be successfully melt extruded out of AV-630 using conventional thermoplastics film extrusion equipment. Films of AV-630 offer certain performance advantages over comparable PEEK film. These include improved toughness and ductility, a higher retention of mechanical integrity at temperatures above 150°C, better acceptance of adhesives and improved flame propagation resistance properties. Ultra-thin films (<15 microns thick) also exhibit a more flexible, less crinkly feel than that of PEEK films at comparable thicknesses. Sub-mil thick films produced from AV-630 can be utilized in a wide range of industrial applications. Typical applications include capacitors, electrical insulation, flexible circuitry substrates, composite film layers, specialty laminates, moisture barriers, liners and aerospace films, such a thermal acoustical insulation blanket bagging materials. Natural: AvaSpire® AV-630 NT&&

Product Description
SupplierSolvay
GenericPAEK
Material StatusCommercial: Active
FeaturesHigh impact resistance,Good Dimensional Stability,Ductility,Flame Characteristics,High Heat Resistance,Fatigue resistance,Solvent resistance
AvailabilitysAfrica & Middle East ,North America,Latin America,Asia Pacific,Europe

Technical Data
PHYSICALNominal valueUnitTest method
Density1.30g/cm³ASTM D792
Melt Flow Rate
400℃,2.16kg7.0g/10minASTM D1238
Water absorption rate
24hr0.20%ASTM D570

IMPACTNominal valueUnitTest method
Impact strength of cantilever beam notch 
91J/mASTM D256
7.0kJ/m²ISO 180
Notched impact strength of cantilever beam无断裂 ASTM D4812 , ISO 180

THERMALNominal valueUnitTest method
Hot deformation temperature
1.8 MPa, annealed, 3.2 mm181ASTM D648
Glass transition temperature158ASTM D3418
Melting peak temperature340ASTM D3418
specific heat DSC
50℃1390J/kg/℃DSC
200℃1960J/kg/℃DSC
Thermal conductivity coefficient0.23W/m/KASTM E1530

Electrical performanceNominal valueUnitTest method
Surface resistivity> 1.9E+17ohmsASTM D257
Volume resistivity6.2E+17ohms·cmASTM D257
Dielectric strength
0.06 mm, amorphous film180kV/mmASTM D149

FLAME CHARACTERISTICSNominal valueUnitTest method
Extreme oxygen index38%ASTM D2863

MECHANICALNominal valueUnitTest method
Rockwell hardness
M-level92 ASTM D785
Tensile modulus 
3300MPaASTM D638
3400MPaISO 527-2/1A/1
tensile strength 
yield89.0MPaISO 527-2/1A/50
92.0MPaASTM D638
Tensile strain 
yield6.0%ASTM D638
yield5.4%ISO 527-2/1A/50
fracture50 to 80%ASTM D638
fracture50 to 80%ISO 527-2/1A/50
Bending modulus 
320MPaASTM D790
3300MPaISO 178
bending strength 
127MPaASTM D790
128MPaISO 178
compressive strength110MPaASTM D695
shear strength79.0MPaASTM D732

Process Conditions
ExtrusionNominal valueUnitTest method
Drying temperature149°C
Drying time4.0hr

Notes
1. Typical properties: these are not to be construed as specifications.
2. 2.0 in/min
3. 2 hours at 200°C
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.