AvaSpire® AV-848 GF30

About
AvaSpire® AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable grades of reinforced PEEK. These include improved dimensional stability, higher stiffness and lower CLTE from 150°C to 240°C, and lower modulus for greater flexibility at room temperature. High temperature AV-848 GF30 provides design engineers with an alternative to reinforced PEEK, specifically in demanding applications that require superior toughness, higher structural integrity, and exceptional chemical resistance. AvaSpire® PAEK can be easily processed using standard thermoplastic melt processing techniques, including injection molding and extrusion. Natural: AvaSpire® AV-848 NT&&

Product Description
SupplierSolvay
GenericPAEK
Material StatusCommercial: Active
FeaturesGood Rigidity,Good Dimensional Stability,Flame Characteristics,High Heat Resistance,Fatigue resistance,Solvent resistance
AvailabilitysAfrica & Middle East ,North America,Latin America,Asia Pacific,Europe
Process MethodsInjection Molding

Technical Data
MECHANICALNominal valueUnitTest method
Tensile modulus10600MPaASTM D638
tensile strength168MPaASTM D638
Tensile strain
fracture2.3%ASTM D638
Bending modulus9900MPaASTM D790
bending strength239MPaASTM D790
compressive strength139MPaASTM D695
shear strength84.8MPaASTM D732

IMPACTNominal valueUnitTest method
Impact strength of cantilever beam notch69J/mASTM D256
Notched impact strength of cantilever beam960J/mASTM D256

THERMALNominal valueUnitTest method
Hot deformation temperature
1.8 MPa, annealed, 3.2 mm257ASTM D648
Glass transition temperature158DSC
Melting peak temperature340ASTM D3418
specific heat DSC
50℃1300J/kg/℃DSC
200℃1700J/kg/℃DSC
Thermal conductivity coefficient0.29W/m/KASTM E1530

Electrical performanceNominal valueUnitTest method
Surface resistivity> 1.9E+17ohmsASTM D257
Volume resistivity1.8E+17ohms·cmASTM D257
Dielectric strength
3 mm18kV/mmASTM D149
Dielectric constant ASTM D150
60 Hz3.74 ASTM D150
1 MHz3.69 ASTM D150
Dissipation factor ASTM D150
60 Hz2.0E-3 ASTM D150
1 MHz6.0E-3 ASTM D150

PHYSICALNominal valueUnitTest method
Density1.53g/cm³ASTM D792
Melt Flow Rate
400℃,2.16kg9.0g/10minASTM D1238
Shrinkage rate ASTM D955
MD:3.2 mm0.20 to 0.40%ASTM D955
TD:3.2 mm0.50 to 0.70%ASTM D955
Water absorption rate
24hr0.10%ASTM D570
Apparent viscosity of melt
400℃,1000 sec^-160.0Pa·sASTM D3835

Process Conditions
injectionNominal valueUnitTest method
Drying temperature149°C
Drying time4.0hr
Barrel rear temperature366°C
Barrel middle temperature371°C
Barrel front temperature377°C
Nozzle temperature382°C
Processing (melt) temperature382 to 404°C
Mold temperature166 to 193°C
Injection speed快速 
Screw compression ratio2.0 : 1.0 to 3.0 : 1.0 

Notes
1. Typical properties: these are not to be construed as specifications.
2. 5″ x 0.5″ x 0.125″ bars
3. 0.20 in/min
4. 2 hours at 200°C
【 Disclaimer 】
Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials.