About |
---|
BIOPLAST 105 is BIOTEC’s trademark for a completely new, plasticizer-free thermoplastic material. As a result of plasticizer absence no material built-up or steam occurs during processing of BIOPLAST 105. The material is extremely suitable for injection moulding, sheet film extrusion and blown film extrusion of completely biodegradable products. The complete biodegradability and other functional properties enable the converter to advance in production areas, which could not be reached with traditional thermoplastic materials.&& |
Product Description | |
---|---|
Generic | 热塑性聚酯 |
Material Status | Commercial: Active |
Features | Good Rigidity,Renewable resources,Low or no water absorption,Good Printability,Biodegradable,Food contact compliance,Moisture resistance,Grease resistance,Gasoline resistance,Good coloring |
Availabilitys | Europe |
Process Methods | Injection Molding |
Technical Data | |||
---|---|---|---|
film | Nominal value | Unit | Test method |
film thickness | |||
test | > 10 | µm | |
tensile strength | ISO 527-3 | ||
MD,23℃,10 µm | 20.0 to 50.0 | MPa | |
TD,23℃,10 µm | 20.0 to 50.0 | MPa | |
Tensile strain | ISO 527-3 | ||
MD, fracture, 10 µ m | 100 to 900 | % | |
TD, fracture, 10 µ m | 100 to 900 | % | |
Water vapor transmittance | |||
10 µm | 70 to 90 | g/m²/24 hr | DIN 53122 |
PHYSICAL | Nominal value | Unit | Test method |
---|---|---|---|
Density | 1.10 to 1.30 | g/cm³ | ISO 1183/A |
Apparent density | 0.75 to 0.83 | g/cm³ | ISO 60 |
Melt Flow Rate | |||
190℃,2.16kg | 3.0 to 11 | g/10min | ISO 1133 |
water content | % | Internal Method | |
Particle size | 3.00 to 4.00 | mm | |
Melt density | 1.00 to 1.20 | g/cm³ | ISO 1133 |
Notes |
---|
【 Disclaimer 】 Guangzhou Soliao Information Technology Co., Ltd. reserves all rights. The information in this data table was obtained from the manufacturer of the material on soliao.com. Soliao.com makes every effort to ensure the accuracy of this data. However, the search company does not assume any responsibility for the uncertainty and consequences caused to users by these data values and suggestions, and strongly recommends verifying the data values with the material supplier before the final selection of materials. |